1. A method of forming a stepped channel potential in a charge-coupled device comprising:
(a) forming a well or a substrate of a first conductivity type;
(b) forming a buried channel of a second conductivity type;
(c) forming a plurality of first gate electrodes;
(d) partially coating the plurality of first gate electrodes with a mask substantially aligned to an edge of each first gate electrode;
(e) producing the stepped channel potential in the buried channel by implanting ions of the first conductivity type with sufficient energy to simultaneously penetrate into the buried channel between the plurality of first gate electrodes and penetrate through the uncoated portions of the plurality of first gate electrodes and into the buried channel; and
(f) forming a plurality of second gate electrodes covering regions of the buried channel between the plurality of first gate electrodes.
2. The method as in claim 1, further comprising prior to (f), producing a larger potential step in the stepped channel potential by implanting ions of the first conductivity type with sufficient energy to penetrate into the buried channel that is between the plurality of first gate electrodes but not penetrate the uncoated portions of the plurality of first gate electrodes.
3. The method as in claim 2, further comprising removing the mask after producing a larger potential step in the stepped channel potential and prior to (f).
4. The method as in claim 1, further comprising removing the mask prior to (f).
5. A method of forming a stepped channel potential in a charge coupled device comprising:
(a) forming a well or a substrate of a first conductivity type;
(b) forming a buried channel of a second conductivity type;
(c) forming a plurality of first gate electrodes;
(d) partially coating the plurality of first gate electrodes with a mask substantially aligned to an edge of each first gate electrode;
(e) producing the stepped channel potential in the buried channel by implanting ions of the first conductivity type with sufficient energy to simultaneously penetrate into the buried channel that is between the plurality of first gate electrodes and penetrate through the uncoated portions of the plurality of first gate electrodes and into the buried channel;
(f) producing a larger potential step in the stepped channel potential by implanting ions of the first conductivity type with sufficient energy to penetrate into the buried channel that is between the plurality of first gate electrodes but not penetrate the uncoated portions of the plurality of first gate electrodes; and
(g) forming a plurality of second gate electrodes covering regions of the buried channel between the first gate electrodes.
6. The method as in claim 5, further comprising removing the mask prior to (g).
7. A method of forming a camera comprising:
(a) providing a camera body;
(b) providing a charge-coupled device in the camera body, the method of providing the charge-coupled device comprising:
(i) forming a well or a substrate of a first conductivity type;
(ii) forming a buried channel of a second conductivity type;
(iii) forming a plurality of first gate electrodes;
(iv) partially coating the plurality of first gate electrodes with a mask substantially aligned to an edge of each first gate electrode;
(v) producing a stepped channel potential in the buried channel by implanting ions of the first conductivity type with sufficient energy to simultaneously penetrate into the buried channel between the plurality of first gate electrodes and penetrate through the uncoated portions of the first gate electrodes and into the buried channel; and
(vi) forming a plurality of second gate electrodes covering regions of the buried channel between the plurality of first gate electrodes.
8. The method as in claim 7, further comprising prior to (vi), producing a larger potential step in the stepped channel potential by implanting ions of the first conductivity type with sufficient energy to penetrate into the buried channel that is between the plurality of first gate electrodes but not penetrate the uncoated portions of the plurality of first gate electrodes.
9. The method as in claim 8, further comprising removing the mask after producing a larger potential step in the stepped channel potential and prior to (vi).
10. The method as in claim 7, further comprising removing the mask prior to (vi).
11. A method of forming a camera comprising:
(a) providing a camera body;
(b) providing a charge-coupled device in the camera body, the method of providing the charge-coupled device comprising:
(i) forming a well or a substrate of a first conductivity type;
(ii) forming a buried channel of a second conductivity type;
(iii) forming a plurality of first gate electrodes;
(iv) partially coating the plurality of first gate electrodes with a mask substantially aligned to an edge of each first gate electrode;
(v) producing a stepped channel potential in the buried channel by, implanting ions of the first conductivity type with sufficient energy to simultaneously penetrate into the buried channel that is between the plurality of first gate electrodes and penetrate through the uncoated portions of the plurality of first gate electrodes and into the buried channel;
(vi) producing a larger potential step in the stepped channel potential by implanting ions of the first conductivity type with sufficient energy to penetrate into the buried channel that is between the plurality of first gate electrodes but not into the uncoated portions of the plurality of first gate electrodes; and
(vii) forming a plurality of second gate electrodes covering regions of the buried channel between the first gate electrodes.
12. The method as in claim 11, further comprising removing the mask prior to (vii).
The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.
1. A manufacturing method of a pixel define layer of a display panel, comprising:
step 1: sequentially forming a photosensitive resin layer and a transparent define layer on a substrate;
step 2: forming an opening of the photosensitive resin layer and an opening of the transparent define layer in a region corresponding to each pixel region of the display panel,
wherein the opening of the transparent define layer is smaller than the opening of the photosensitive resin layer so as to form a fill region with a wide lower portion and a narrow upper portion,
wherein the step 2 includes:
forming a second photosensitive resin layer on the transparent define layer, and performing a first exposure so that both the second photosensitive resin layer and the photosensitive resin layer under the second photosensitive resin layer in the region corresponding to each pixel region of the display panel are exposed;
removing the second photosensitive resin layer;
forming a third photosensitive resin layer, and performing a second exposure so that the third photosensitive resin layer in the region corresponding to each pixel region of the display panel is exposed, wherein an exposure region formed by the second exposure is smaller than an exposure region formed by the first exposure;
removing the third photosensitive resin layer in the exposure region formed by the second exposure, so as to expose the transparent define layer in this region;
removing the exposed transparent define layer, so as to form an opening of the transparent define layer in the region corresponding to each pixel region of the display panel; and
removing the photosensitive resin layer in the exposure region formed by the first exposure, so as to form an opening of the photosensitive resin layer in the region corresponding to each pixel region of the display panel.
2. The method according to claim 1, wherein the exposure region formed by the second exposure is smaller than the exposure region formed by the first exposure refers to that:
a center of the exposure region formed by the second exposure coincide with a center of the exposure region formed by the first exposure;
a shape of the exposure region formed by the second exposure is the same as a shape of the exposure region formed by the first exposure; and
an area of the exposure region formed by the second exposure is smaller than an area of the exposure region formed by the first exposure.
3. The method according to claim 1, wherein the first exposure and the second exposure use a same mask plate, and a distance between the mask plate and the substrate in the first exposure is smaller than the distance between the mask plate and the substrate in the second exposure.
4. The method according to claim 1, wherein the transparent define layer is made of a hydrophobic material.
5. The method according to claim 4, wherein the transparent define layer is made of silicon nitride.
6. The method according to claim 1, wherein the transparent define layer is made of a hydrophilic material.
7. The method according to claim 6, wherein the transparent define layer is made of silicon oxide.
8. A manufacturing method of a pixel define layer of a display panel, comprising:
step 1: sequentially forming a photosensitive resin layer and a transparent define layer on a substrate;
step 2: forming an opening of the photosensitive resin layer and an opening of the transparent define layer in a region corresponding to each pixel region of the display panel, wherein the opening of the transparent define layer is smaller than the opening of the photosensitive resin layer so as to form a fill region with a wide lower portion and a narrow upper portion,
wherein the step 2 includes:
forming a second photosensitive resin layer on the transparent define layer, and performing a first exposure so that both the second photosensitive resin layer and the photosensitive resin layer under the second photosensitive resin layer in the region corresponding to each pixel region of the display panel are exposed;
removing the second photosensitive resin layer, and at the same time, removing the photosensitive resin layer in an exposure region formed by the first exposure, so as to form an opening of the photosensitive resin layer in the region corresponding to each pixel region of the display panel;
forming a third photosensitive resin layer, and performing a second exposure so that the third photosensitive resin layer in the region corresponding to each pixel region of the display panel is exposed, wherein an exposure region formed by the second exposure is smaller than the exposure region formed by the first exposure;
removing the third photosensitive resin layer in the exposure region formed by the second exposure, so as to expose the transparent define layer in this region;
removing the exposed transparent define layer, so as to form an opening of the transparent define layer in the region corresponding to each pixel region of the display panel.
9. The method according to claim 8, wherein the exposure region formed by the second exposure is smaller than the exposure region formed by the first exposure refers to that:
a center of the exposure region formed by the second exposure coincide with a center of the exposure region formed by the first exposure; a shape of the exposure region formed by the second exposure is the same as a shape of the exposure region formed by the first exposure; and an area of the exposure region formed by the second exposure is smaller than an area of the exposure region formed by the first exposure.
10. The method according to claim 8, wherein the first exposure and the second exposure use a same mask plate, and a distance between the mask plate and the substrate in the first exposure is smaller than the distance between the mask plate and the substrate in the second exposure.
11. The method according to claim 8, wherein the transparent define layer is made of a hydrophobic material.
12. The method according to claim 11, wherein the transparent define layer is made of silicon nitride.
13. The method according to claim 8, wherein the transparent define layer is made of a hydrophilic material.
14. The method according to claim 13, wherein the transparent define layer is made of silicon oxide.