What is claimed is:
1. A silver halide emulsion containing a dispersion medium and silver halide grains, wherein the silver halide grains have a variation coefficient of projected area diameters of 30% or less and 50% or more of the total projected area of the silver halide grains is occupied by silver halide grains satisfying the following requirements (a), (b), (c) and (d):
(a) a hexagonal tabular silver halide grain having a smooth (111) face as a principal plane;
(b) the silver iodide content is 7 mol % or more;
(c) the projected area diameter is 3 m or more; and
(d) the aspect ratio is 8 or more.
2. The silver halide emulsion according to claim 1, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (e) below as well as requirements of from (a) to (d):
(e) the ratios of the areas of (100) faces relative to the average area of the side surface calculated from the average projected area and the average thickness of all the grains are 50% or more.
3. The silver halide emulsion according to claim 1, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (f) below as well as requirements of from (a) to (d):
(f) the equivalent-sphere diameter is 1.2 m or more.
4. The silver halide emulsion according to claim 2, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (f) below as well as requirements of from (a) to (e):
(f) the equivalent-sphere diameter is 1.2 m or more.
5. The silver halide emulsion according to claim 1, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (g) below as well as requirements of from (a) to (d):
(g) the grains have at least ten dislocation lines per grain.
6. The silver halide emulsion according to claim 2, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (g) below as well as requirements of from (a) to (e):
(g) the grains have at least ten dislocation lines per grain.
7. The silver halide emulsion according to claim 3, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (g) below as well as requirements of from (a) to (d) and (f):
(g) the grains have at least ten dislocation lines per grain.
8. The silver halide emulsion according to claim 4, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (g) below as well as requirements of from (a) to (f):
(g) the grains have at least ten dislocation lines per grain.
9. The silver halide emulsion according to claim 1, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (h) below as well as requirements of from (a) to (d):
(h) the grains have, in their vertex portions andor peripheral portions andor principal plane portions, at least one epitaxial junction per grain.
10. The silver halide emulsion according to claim 2, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (h) below as well as requirements of from (a) to (e):
(h) the grains have, in their vertex portions andor peripheral portions andor principal plane portions, at least one epitaxial junction per grain.
11. The silver halide emulsion according to claim 3, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (h) below as well as requirements of from (a) to (d) and (f):
(h) the grains have, in their vertex portions andor peripheral portions andor principal plane portions, at least one epitaxial junction per grain.
12. The silver halide emulsion according to claim 4, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (h) below as well as requirements of from (a) to (f):
(h) the grains have, in their vertex portions andor peripheral portions andor principal plane portions, at least one epitaxial junction per grain.
13. The silver halide emulsion according to claim 5, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (h) below as well as requirements of from (a) to (d) and (g):
(h) the grains have, in their vertex portions andor peripheral portions andor principal plane portions, at least one epitaxial junction per grain.
14. The silver halide emulsion according to claim 6, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (h) below as well as requirements of from (a) to (e) and (g):
(h) the grains have, in their vertex portions andor peripheral portions andor principal plane portions, at least one epitaxial junction per grain.
15. The silver halide emulsion according to claim 7, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (h) below as well as requirements of from (a) to (d), (f) and (g):
(h) the grains have, in their vertex portions andor peripheral portions andor principal plane portions, at least one epitaxial junction per grain.
16. The silver halide emulsion according to claim 8, wherein the silver halide grains occupying 50% or more of the total projected area satisfy requirement (h) below as well as requirements of from (a) to (g):
(h) the grains have, in their vertex portions andor peripheral portions andor principal plane portions, at least one epitaxial junction per grain.
The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.
1. A method of forming an insulating material, the method comprising:
forming an interface layer;
removing a portion of the interface layer;
annealing the interface layer;
exposing the annealed interface layer to nitrogen; and
forming a dielectric material over the interface layer.
2. The method according to claim 1, wherein exposing the interface layer to nitrogen comprises: exposing the interface layer to a nitrogen-containing gas or liquid, exposing the interface layer to a plasma nitridation process, exposing the interface layer to a thermal nitridation process, or exposing the interface layer to an implantation process.
3. The method according to claim 1, wherein forming the interface layer comprises forming the interface layer by thermal oxidation, atomic layer deposition (ALD), chemical vapor deposition (CVD), physical vapor deposition (PVD), pulsed laser deposition (PLD), or molecular beam epitaxy (MBE).
4. The method according to claim 1, wherein forming the interface layer comprises forming an interface layer comprising SiO2, LaAlO3, La(RE)O3, or Sc(RE)O3, wherein RE comprises a rare earth metal.
5. The method according to claim 1, wherein forming the interface layer comprises forming an interface layer including a rare earth metal comprising Scandium (Sc), Yttrium (Y), Lanthanum (La), Cerium (Ce), Praseodymium (Pr), Neodymium (Nd), Promethium (Pm), Samarium (Sm), Europium (Eu), Gadolinium (Gd), Terbium (Tb), Dysprosium (Dy), Holmium (Ho), Erbium (Er), Thulium (Tm), Ytterbium (Yb), andor Lutetium (Lu).
6. The method according to claim 1, wherein annealing the interface layer comprises subjecting the interface layer to a high temperature rapid thermal anneal at a temperature of between about 1,000 and 1,250 degrees C.
7. The method according to claim 1, wherein forming the dielectric material comprises forming HfOx, ZrOx, LaOx, HfSiO, ZrSiO, LaSiO, HfSixOyNz, ZrSixOyNz, LaSixOyNz, laminates thereof, multiple layers thereof, one or more rare earth element, an oxide of at least one rare earth element, or at least one rare earth element and at least one transition metal.
8. A method of fabricating a semiconductor device, the method comprising:
providing a workpiece;
forming an interface layer directly onto a top surface of the workpiece, said interface layer having a thickness no greater than 5 nm;
removing a top portion of the interface layer to reduce the remaining thickness of said interface layer to 1 nm or less;
annealing the workpiece at a temperature of greater than about 1,000 degrees C. subsequent to removing a top portion; and
forming a dielectric material over the interface layer.
9. The method according to claim 8, wherein removing a portion of the interface layer comprises removing about one half or greater of the interface layer.
10. The method according to claim 8, wherein annealing the workpiece comprises a flash anneal process, a spike anneal process, or a rapid thermal anneal (RTA) process.
11. The method according to claim 8, wherein forming the interface layer comprises a steam based thermal oxide deposition process.
12. The method according to claim 8, wherein forming the interface layer comprises forming a ternary oxide.
13. The method of claim 9 further comprising exposing the interface layer to nitrogen subsequent to said annealing its interface.
14. A method of forming an insulating material, the method comprising: forming an interface layer directly onto the surface of a workpiece, said interface layer having a thickness no greater than 5 nm;
removing a top portion of the interface layer to reduce the thickness of said interface layer to 1 nm or less;
annealing the interface layer subsequent to removing a top portion of the interface layer; and
forming a dielectric material over the interface layer.
15. A method of fabricating a semiconductor device, the method comprising:
providing a workpiece;
cleaning the workpiece;
forming an interface layer over the workpiece;
removing a portion of the interface layer so that the thickness of the interface layer comprises about 1 nm or less;
annealing the workpiece to densify the interface layer;
forming a dielectric material over the interface layer, wherein the interface layer and the dielectric material comprise an insulating material; and
forming a conductive material over the dielectric material.
16. The method according to claim 15, wherein forming the dielectric material comprises forming a material having a thickness of about 15 nm or less.
17. The method according to claim 15, further comprising nitriding the interface layer after annealing the workpiece, forming a nitrided surface on the interface layer.
18. The method according to claim 17, wherein nitriding the interface layer comprises a nitridation process in a N2 or NH3 ambient at a temperature of between about 550 to 800\xb0 C. for about 10 to 60 seconds, or a uniform surface nitridation process in a plasma nitridation chamber.
19. The method according to claim 15, wherein forming the dielectric material comprises forming a dielectric material having a dielectric constant (k) greater than about 3.9.
20. The method according to claim 15, wherein forming the interface layer and forming the dielectric material comprise forming an insulating material comprising a gate dielectric of a transistor or a capacitor dielectric of a capacitor.
21. The method according to claim 15, wherein forming the conductive material comprises forming TiN, TaN, Ru, RuO2, TiSiN, TaSiN, HfSiN, TiHfN, TiCN, TaCN, TiXN, AlN, RE1RE2N, polysilicon, andor multiple layers or combinations thereof, wherein X comprises a rare earth element, wherein RE1RE2N comprises a nitride of a first rare earth element RE1 and a second rare earth element RE2, and wherein the second rare earth element comprises a different rare earth element than the first rare earth element.