What is claimed is:
1. A semiconductor diode comprising:
a first stage having a first semiconductor layer and two conductive contacts; and
a second stage having a second semiconductor layer and two conductive contacts;
wherein one of the conductive contacts of the first stage and one of the conductive contacts of the second stage are joined together.
2. The diode of claim 1, wherein the two contacts on each stage are formed from different materials.
3. The diode of claim 1, wherein one of the contacts on each stage includes a metallic material having a low metal work function.
4. The diode of claim 3, wherein the metallic material is selected from a group including gold, palladium, platinum, and rhenium.
5. The diode of claim 1, wherein one of the contacts on each stage includes a metallic material having a high metal work function.
6. The diode of claim 5, wherein the metallic material is selected from a group including titanium and titanium aluminum.
7. The diode of claim 1, wherein one of the contacts on each stage forms an ohmic contact.
8. The diode of claim 1, wherein one of the contacts on each stage forms a Schottky contact.
9. The diode of claim 1, wherein the semiconductor layers include a nitride-based semiconductor material.
10. The diode of claim 9, wherein the semiconductor material is selected from a group including gallium nitride and aluminum gallium nitride.
11. The diode of claim 1, wherein the semiconductor layers include a carbide-based semiconductor material.
12. The diode of claim 11, wherein the semiconductor material includes silicon carbide.
13. The diode of claim 1, wherein the semiconductor materials used to form the semiconductor layers vary from stage to stage.
14. The diode of claim 1, wherein at least one of the semiconductor layers has a varying doping concentration.
The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.
1. A method for reacting oxygen-containing polymers to form hydrogen and alkali metal carbonates, comprising:
bringing polymers comprising carbon, hydrogen and oxygen atoms with and without further atoms into intimate contact with a molten mixture of alkali metal hydroxide and alkali metal carbonate;
carrying out the reaction while avoiding direct contact of the interior of the employed reactor above the molten mixture with the oxygen of the atmosphere; and
separating off the resulting hydrogen and crystallizing out and separating off the resulting alkali metal carbonate;
wherein at least a quantity of alkali metal hydroxide is made available, and a concentration of alkali metal hydroxide is maintained in the reaction mixture during the reaction, which are sufficient to start and maintain an exothermic reaction of alkali metal hydroxide together with the oxygen-containing polymers.
2. The method according to claim 1 wherein an excess of melt is initially charged to ensure an excess of alkali metal hydroxide based on the polymer.
3. The method according to claim 1 wherein further alkali metal hydroxide is added.
4. The method according to claim 1 wherein the reaction is carried out in a melt at a constant temperature and at a constant composition, the temperature and the composition being on one point of the liquidus line of the temperature-composition diagram.
5. The method according to claim 4 wherein the reaction temperature is varied from 1 to 10\xb0 C. along the liquidus line.
6. The method according to claim 1, wherein the polymers are used in crushed form.
7. The method according to claim 1, wherein the method is carried out in a system which is sealed off from ambient air.
8. The method according to claim 1, wherein a molten mixture in the form of a saturated solution of alkali metal carbonate in alkali metal hydroxide is used.
9. The method according to claim 1, wherein sodium hydroxide is used as alkali metal hydroxide and sodium carbonate as alkali metal carbonate.
10. The method according to claim 1, wherein a molten mixture of eutectic composition is used.
11. The method according to claim 1, wherein a melt composition in the vicinity of the eutecticum is used.
12. The method according to claim 11 wherein one or other component is present in the melt at a concentration which is up to 0.5 mol % higher than that corresponding to the eutecticum.
13. The method according to claim 9 wherein a molten mixture is used in which the fraction of sodium carbonate in the molten mixture is in the range from 6 to 40 mol %.
14. The method according to claim 1, wherein a temperature gradient is established in the reaction vessel.
15. The method according to claim 1 wherein the polymers are temporarily added into a melt composition which is above the liquidus line and the addition of further alkali metal hydroxide is only resumed once the melt has reached the liquidus line by virtue of the carbonate formed.
16. The method according to claim 1, wherein during the reaction, the composition of the molten mixture is shifted into andor temporarily maintained in the region above the liquidus line by increased addition of alkali metal hydroxide and the addition of alkali metal hydroxide is interrupted until the solidousliquidus line is reached again.
17. The method according to claim 1, wherein polymers or polymer mixtures from the group consisting of polyesters, polycarbonates, polyethers, polyacetals, epoxy resins, polylactones, polylactides, polyglycolides, polyacrylates, polyvinyl acetate, biopolymers, wood, cellulose, lignin, cutin and pectin are used for the reaction.
18. The method according to claim 1, wherein the polymers used comprise still other constituents being reinforcing fibers, fillers, customary additives, or are present as composite materials.
19. The method according to claim 1, wherein oxygen is added to the melt in free or bound form, in particular in the case of polymers where the ratio of oxygen atoms to carbon atoms is less than 1 and which require oxygen for complete oxidation of the carbon atoms, the oxygen in free form being introduced underneath the surface of the melt and the oxygen in bound form being introduced above or underneath the surface of the melt.
20. The method according to claim 19 wherein the oxygen in bound form is introduced in the form of formic acid, oxalic acid, water or carbon dioxide.
21. The method according to claim 1, wherein the method is carried out continuously.
22. The method according to claim 9 wherein a molten mixture is used in which the fraction of sodium carbonate in the molten mixture is in the range from 6 to 20 mol %.
23. The method according to claim 9 wherein a molten mixture is used in which the fraction of sodium carbonate in the molten mixture is in the range from 6 to 10 mol %.