1. A method for selectively etching a high k layer with respect to a silicon based material, comprising:
placing the high k layer into an etch chamber;
providing an etchant gas into the etch chamber, wherein the etchant gas comprises H2; and
generating a plasma from the etchant gas to selectively etch the high k layer with respect to the silicon based material.
2. The method, as recited in claim 1, wherein the high k dielectric layer is an oxide layer.
3. The method, as recited in claim 2, wherein the etchant gas further comprises a halogen containing component.
4. The method, as recited in claim 3, wherein the etchant gas further comprises a noble gas.
5. The method, as recited in claim 1, wherein the etchant gas further comprises BCl3 and an inert gas.
6. The method, as recited in claim 5, wherein the etchant gas has a volume H2 to BCl3 flow ration between 0.2-5:1.
7. The method, as recited in claim 6, wherein the etchant gas has a volume inert gas flow of less than 500 sccm.
8. The method, as recited in claim 7, wherein the etchant gas further comprises Cl2.
9. The method, as recited in claim 8, wherein the etchant gas has a volume Cl2 to BCl3 flow ratio between 0-0.5:1.
10. The method, as recited in claim 1, wherein the etchant gas further comprises BCl3 and Cl2.
11. The method, as recited in claim 10, wherein the etchant gas has a volume H2 to BCl3 flow ration between 0.2-5:1.
12. The method, as recited in claim 11, wherein the etchant gas has a volume Cl2 to BCl3 flow ratio between 0-0.5:1.
13. The method, as recited in claim 12, wherein the silicon based material is at least one of silicon and silicon nitride and wherein the high k layer is at least one of Hf silicate, HfO2, Zr silicate, ZrO2, Al2O3, La2O3, SrTiO3, SrZrO3, TiO2, and Y2O3.
14. The method, as recited in claim 13, wherein the silicon based material forms a layer, further comprising etching the silicon based material layer subsequent to selectively etching the high k layer.
15. A semiconductor devices formed by the method of claim 1.
16. A method for etching a stack with a high k layer over a silicon based layer, comprising:
placing the stack into an etch chamber;
selectively etching the high k layer with respect to the silicon based layer, comprising:
providing a high k layer etchant gas into the etch chamber, wherein the high k layer etchant gas comprises H2; and
generating a plasma from the high k layer etchant gas to selectively etch the high k layer with respect to the silicon based layer;
stopping the selectively etching the high k layer; and
selectively etching the silicon based layer with respect to the high k layer.
17. The method, as recited in claim 16, wherein the high k layer etchant gas further comprises BCl3 and Cl2 and wherein the silicon based layer is formed of a silicon based material comprising at least one of silicon and silicon nitride.
18. The method, as recited in claim 17, wherein the high k layer etchant gas has a volume H2 to BCl3 flow ration between 0.2-5:1 and wherein the silicon based material is silicon.
19. The method, as recited in claim 18, wherein the high k layer etchant gas has a volume Cl2 to BCl3 flow ratio between 0-0.5:1.
20. An apparatus for forming flash memory with a high k dielectric layer over a silicon based layer, comprising:
a plasma processing chamber, comprising:
a chamber wall forming a plasma processing chamber enclosure;
a substrate support for supporting a substrate within the plasma processing chamber enclosure;
a pressure regulator for regulating the pressure in the plasma processing chamber enclosure;
at least one electrode for providing power to the plasma processing chamber enclosure for sustaining a plasma;
a gas inlet for providing gas into the plasma processing chamber enclosure; and
a gas outlet for exhausting gas from the plasma processing chamber enclosure;
a gas source in fluid connection with the gas inlet, comprising;
an H2 gas source;
a BCl3 gas source; and
a Cl2 gas source;
a controller controllably connected to the gas source and the at least one electrode, comprising:
at least one processor; and
computer readable media comprising:
computer readable code for selectively etching the high k layer with respect to the silicon based layer, comprising:
computer readable code for providing H2 from the H2 gas source;
computer readable code for providing BCl3 from the BCl3 gas source;
computer readable code for providing Cl2 from the Cl2 gas source; and
computer readable code for generating a plasma from the H2, BCl3, and Cl2 to selectively etch the high k layer with respect to the silicon based layer;
computer readable code to stop the selectively etching the high k layer with respect to the silicon based layer; and
computer readable code for selectively etching the silicon based with respect to the high k layer.
The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.
What is claimed is:
1. A semiconductor device comprising:
a Cu film provided above a main surface of a semiconductor substrate and used as a wiring;
an intermediate layer formed at least on the Cu film; and
an Al film formed on the intermediate layer and used as a pad;
wherein the intermediate layer comprises a refractory metal nitride film and a refractory metal film formed on the refractory metal nitride film.
2. The semiconductor device according to claim 1, wherein the intermediate layer has a first portion which contacts the Cu film and a second portion which does not contact the Cu film, and an insulating film contacts the second portion.
3. The semiconductor device according to claim 1, wherein the refractory metal film contains at least one refractory metal and the refractory metal nitride film contains at least one refractory metal that is identical to the at least one refractory metal contained in the refractory metal film.
4. The semiconductor device according to claim 1, wherein the refractory metal film contains at least one metal selected from the group consisting of Ta, Nb, Ti, W and V, and the refractory metal nitride film contains at least one metal selected from the group consisting of Ta, Nb, Ti, W and V.
5. A semiconductor device comprising:
a Cu film provided above a main surface of a semiconductor substrate and used as a wiring;
an intermediate layer formed at least on the Cu film; and
an Al film formed on the intermediate layer and used as a pad;
wherein the intermediate layer comprises a refractory metal film and a refractory metal nitride film formed on the refractory metal film.
6. The semiconductor device according to claim 5, wherein the intermediate layer has a first portion which contacts the Cu film and a second portion which does not contact the Cu film, and an insulating film contacts the second portion.
7. The semiconductor device according to claim 5, wherein the refractory metal film contains at least one refractory metal and the refractory metal nitride film contains at least one refractory metal that is identical to the at least one refractory metal contained in the refractory metal film.
8. The semiconductor device according to claim 5, wherein the refractory metal film contains at least one metal selected from the group consisting of Ta, Nb, Ti, W and V, and the refractory metal nitride film contains at least one metal selected from the group consisting of Ta, Nb, Ti, W and V.
9. A semiconductor device comprising:
a Cu film provided above a main surface of a semiconductor substrate and used as a wiring;
an intermediate layer formed at least on the Cu film; and
an Al film formed on the intermediate layer and used as a pad;
wherein the intermediate layer comprises a first refractory metal film, a refractory metal nitride film formed on the first refractory metal film, and a second refractory metal film formed on the refractory metal nitride film.
10. The semiconductor device according to claim 9, wherein the intermediate layer has a first portion which contacts the Cu film and a second portion which does not contact the Cu film, and an insulating film contacts the second portion.
11. The semiconductor device according to claim 9, wherein the first refractory metal film contains at least one refractory metal, the refractory metal nitride film contains at least one refractory metal that is identical to the at least one refractory metal contained in the first refractory metal film, and the second refractory metal film contains at least one refractory metal that is identical to the at least one refractory metal contained in the first refractory metal film.
12. The semiconductor device according to claim 9, wherein the first refractory metal film contains at least one metal selected from the group consisting of Ta, Nb, Ti, W and V, the refractory metal nitride film contains at least one metal selected from the group consisting of Ta, Nb, Ti, W and V, and the second refractory metal film contains at least one metal selected from the group consisting of Ta, Nb, Ti, W and V.