1. A shelf-stable composition for use in dry mix applications comprising a water redispersible polymer powder (RDP) composition containing B) a multi-stage acrylic copolymer RDP and A) from 0.1 to 7.5 wt. %, based on the total weight of A) and B), of a dry anionic associative thickener selected from a hydrophobically modified alkali swellable acrylic emulsion copolymer (HASE), an alkali swellable acrylic emulsion copolymer, and mixtures thereof, the multi-stage acrylic copolymer RDP B) having a calcium methacrylate salt group containing alkali-soluble resin outer stage and one or more inner stage, the RDP further containing each of one or more nucleating agent having a boiling point of 150\xb0 C. to 500\xb0 C. and a water solubility of 3.5% or less, and one or more colloidal stabilizer,
wherein when the multi-stage acrylic copolymer is dispersed in water the one or more inner stage comprises an acrylic (co)polymer having a glass transition temperature (Tg) of from \u221210 to 15\xb0 C. calculated using the Fox equation,
and the weight ratio of the alkali-soluble resin outer stage to the one or more inner stage(s) ranges from 1:19 to 2:3 and
the dry anionic associative thickener, the colloidal stabilizer, the nucleating agent and the multi-stage acrylic copolymer are contained in the same particle.
2. The shelf-stable composition for use in dry mix applications as claimed in claim 1, wherein the amount of the A) dry anionic associative thickener ranges from 0.25 to 2 wt. %, based on the total weight of A) and B).
3. The shelf-stable composition for use in dry mix applications as claimed in claim 1, wherein the A) dry anionic associative thickener is a hydrophobically modified alkali swellable acrylic emulsion copolymer (HASE).
4. The shelf-stable composition for use in dry mix applications as claimed in claim 1, wherein the B) multi-stage acrylic copolymer RDP contains, in copolymerized form, a crosslinking agent in the range of 0.05 to 2.0% wt. %, based on the total weight of the monomers used to make the copolymer.
5. The shelf-stable composition for use in dry mix applications as claimed in claim 1, wherein the B) multi-stage acrylic copolymer RDP contains a chain transfer agent residue, in the range of from 0.05 to 1.0 wt. %, based on the total weight of the monomers and chain transfer agents used to make the copolymer.
6. The shelf-stable composition for use in dry mix applications as claimed in claim 1, wherein the B) multi-stage acrylic copolymer RDP contains from 0.1 to 15 wt. % of the one or more colloidal stabilizer, per 100 weight parts multi-stage acrylic copolymer solids.
7. The shelf-stable composition for use in dry mix applications as claimed in claim 6, wherein the colloidal stabilizer is a poly(vinyl alcohol) (PVOH).
8. The composition as claimed in claim 1, wherein the B) multi-stage acrylic copolymer RDP further comprises one or more hydrophobic agent.
9. The shelf-stable composition for use in dry mix applications as claimed in claim 1, wherein the B) multi-stage acrylic copolymer RDP further comprises one or more anti-caking aid.
10. The shelf-stable composition for use in dry mix applications as claimed in claim 1, further comprising an inorganic dry material selected from a cementitious material and a non-cementitious material.
11. A method of making a water redispersible polymer powder composition comprising providing an aqueous dispersion containing one or more colloidal stabilizer, and a multi-stage acrylic copolymer having an alkali-soluble resin outer stage comprising methacrylic acid groups and one or more inner stage, one or more nucleating agent having a boiling point of 150\xb0 C. to 500\xb0 C. and a water solubility of 3.5% or less, wherein when the multi-stage acrylic copolymer is dispersed in water the one or more inner stage comprises an acrylic (co)polymer having a glass transition temperature (Tg) of from \u221210 to 15\xb0 C., calculated using the Fox equation, and atomizing the resulting composition in the presence of from 0.75 to 3 wt. % of calcium hydroxide or aqueous lime, based on the total weight of the multi-stage acrylic copolymer solids, to form a water redispersible polymer powder, providing separately an aqueous mixture of an anionic associative thickener selected from a hydrophobically modified alkali swellable acrylic emulsion copolymer (HASE), an alkali swellable acrylic emulsion copolymer or mixtures thereof in the amount of from 0.1 to 7.5 wt. %, based on the total weight of solids in the aqueous mixture and the aqueous dispersion, atomizing the aqueous mixture to form a dry anionic associative thickener and blending the dry anionic associative thickener and the water redispersible polymer powder.
The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.
1. A solid oxide fuel cell supplied with a fuel gas and an oxidant gas, the solid oxide fuel cell comprising:
an electrolyte-supported or electrode-supported single cell having a anode, an electrolyte, and an cathode in this order;
a conductive support substrate supporting the single cell, and having a supply path for the fuel gas or the oxidant gas; and
a conductive welding layer with gas permeability, the welding layer being sandwiched between the single cell and the support substrate, and welded to the single cell and the support substrate.
2. A solid oxide fuel cell supplied with a fuel gas and an oxidant gas, the solid oxide fuel cell comprising:
an electrolyte-supported or electrode-supported single cell having a anode, an electrolyte, and an cathode in this order;
a pair of conductive support substrates sandwiching the single cell on a anode side and an cathode side, and having a supply path for the fuel gas or the oxidant gas; and
conductive welding layers with gas permeability, each welding layer being sandwiched between the single cell and each support substrate, and welded to the single cell and the support substrate.
3. The solid oxide fuel cell according to claim 1 or 2, wherein the welding layer has a predetermined pattern communicating the single cell and the support substrate.
4. The solid oxide fuel cell according to claim 1 or 2, wherein the welding layer is made of a sheet material.
5. The solid oxide fuel cell according to claim 1 or 2, wherein the welding layer comprises silver or a compound containing silver.
6. The solid oxide fuel cell according to claim 1 or 2, wherein the welding layer has a melting point of 1,200\xb0 C. or less.
7. The solid oxide fuel cell according to claim 1 or 2, wherein the support substrate has at least one through-hole, the through-hole being communicating and forming the supply path.
8. The solid oxide fuel cell according to claim 1 or 2, wherein the support substrate is porous, and a plurality of pores in the support substrate form the supply path.
9. A solid oxide fuel cell comprising:
an electrolyte-supported or electrode-supported single cell having a anode, an electrolyte, and an cathode in this order;
a support substrate supporting the single cell, and having at least one through-hole;
a porous conductive collector, the collector filling the through-hole in the support substrate, and having a thickness equal to or greater than that of the support substrate; and
a conductive welding layer with gas permeability, the welding layer being sandwiched between the single cell and the support substrate, and welded to the single cell and the support substrate.
10. A solid oxide fuel cell comprising:
an electrolyte-supported or electrode-supported single cell having a anode, an electrolyte, and an cathode in this order;
a pair of conductive support substrates sandwiching the single cell on a anode side and an cathode side, and having at least one through-hole;
a porous conductive collector, the collector filling the through-hole in each of the support substrates, and having a thickness equal to or greater than that of the support substrate; and
a conductive welding layer with gas permeability, the welding layer being sandwiched between the single cell and the support substrate, and welded to the single cell and the support substrate.
11. The solid oxide fuel cell according to claim 9 or 10, wherein the welding layer has a predetermined pattern communicating the single cell and the support substrate.
12. The solid oxide fuel cell according to claim 9 or 10, wherein the welding layer is made of a sheet material.
13. The solid oxide fuel cell according to claim 9 or 10, wherein the welding layer comprises silver or a compound containing silver.
14. The solid oxide fuel cell according to claim 9 or 10, wherein the welding layer has a melting point of 1,200\xb0 C. or less.
15. A method for manufacturing a solid oxide fuel cell comprising the steps of:
preparing an electrolyte-supported or electrode-supported single cell having a anode, an electrolyte, and an cathode in this order;
preparing a conductive support substrate for supporting the single cell;
forming at least one through-hole in the support substrate;
forming a conductive welding layer with gas permeability on at least one of the support substrate and the single cell; and
laminating the support substrate and the single cell so that the welding layer is sandwiched therebetween, and melting the welding layer to thereby weld the melting layer to the support substrate and the single cell.
16. A method for manufacturing a solid oxide fuel cell comprising the steps of:
preparing an electrolyte-supported or electrode-supported single cell having a anode, an electrolyte, and an cathode in this order;
preparing a support substrate for supporting the single cell;
forming at least one through-hole in the support substrate;
forming a conductive welding layer with gas permeability on at least one of the support substrate and the single cell;
laminating the support substrate and the single cell so that the welding layer is sandwiched therebetween, and melting the welding layer to thereby weld the melting layer to the support substrate and the single cell; and
forming a porous collector so as to fill the through-hole in the support substrate.
17. A method for manufacturing a solid oxide fuel cell comprising the steps of:
preparing an electrolyte-supported or electrode-supported single cell having a anode, an electrolyte, and an cathode in this order;
preparing a conductive and porous support substrate for supporting the single cell;
forming a conductive welding layer with gas permeability on at least one of the support substrate and the single cell; and
laminating the support substrate and the single cell so that the welding layer is sandwiched therebetween, and melting the welding layer to thereby weld the melting layer to the support substrate and the single cell.
18. The method according to any one of claims 15 to 17, wherein the welding layer has a predetermined pattern communicating the single cell and the support substrate.
19. The method according to any one of claims 15 to 17, wherein the welding layer is made of a sheet material.
20. A method for manufacturing a solid oxide fuel cell comprising the steps of:
preparing an electrolyte-supported or electrode-supported single cell having a anode, an electrolyte, and an cathode in this order;
preparing two conductive support substrates for supporting the single cell;
forming at least one through-hole in each of the support substrates;
forming conductive welding layers with gas permeability, each welding layer being formed between each of the support substrates and the single cell; and
laminating the support substrates and the single cell so that the two support substrates sandwich the single cell, and each welding layer is sandwiched between each support substrate and the single cell, and melting the welding layers to thereby weld the welding layers to the respective support substrates and the single cell.
21. A method for manufacturing a solid oxide fuel cell comprising:
preparing an electrolyte-supported or electrode-supported single cell having a anode, an electrolyte, and an cathode in this order;
preparing two support substrates for supporting the single cell;
forming at least one through-hole in each of the support substrates;
forming conductive welding layers with gas permeability, each welding layer being formed between each of the support substrates and the single cell;
laminating the two support substrates and the single cell so that the support substrates sandwich the single cell, and each welding layer is sandwiched between each support substrate and the single cell, and melting the welding layers to thereby weld the welding layers to the respective support substrates and the single cell; and
forming a porous collector so as to fill the through-hole in each of the support substrates.
22. A method for manufacturing a solid oxide fuel cell comprising the steps of:
preparing an electrolyte-supported or electrode-supported single cell having a anode, an electrolyte, and an cathode in this order;
preparing two conductive and porous support substrates for supporting the single cell;
forming conductive welding layers with gas permeability, each welding layer being formed between each of the support substrates and the single cell; and
laminating the two support substrates and the single cell so that the support substrates sandwich the single cell, and each welding layer is sandwiched between each support substrate and the single cell, and melting the welding layers to thereby weld the welding layers to the respective support substrates and the single cell.
23. The method according to any one of claims 20 to 22, wherein the step of forming welding layers comprises forming a welding layer on at least one of opposing surfaces of each support substrate and the single cell.
24. The method according to any one of claims 20 to 22, wherein each of the welding layers has a predetermined pattern communicating the single cell and the support substrate.
25. The method according to any one of claims 20 to 22, wherein the welding layer is made of a sheet material.