1. A method for metallizing a plastic surface, the plastic comprising a supporting material and an electroless plating promoter, the method comprising the steps of:
1) gasifying the plastic surface to expose the electroless plating promoter; and
2) electroless plating a layer of copper or nickel on the plastic surface, followed by electroplating or a second electroless plating to form a metallized layer on the plastic surface.
2. The method according to claim 1, wherein the electroless plating promoter includes one or more members selected from a group consisting of:
(a) oxides of the metal elements selected from Co, Ni, Ag;
(b) silicate, borate or oxalate of metal elements selected from Co, Ni, Cu;
(c) hydrogenation catalysts having one or more metal elements selected from Co, Ni, Cu, Ag;
(d) ABO2 type composite oxides having a delafossite structure, in which A is one of metal elements selected from Co, Ni, Cu, B is an element selected from a group consisting of Ni, Mn, Cr, Al and Fe where A, B are different; and
(e) multicomponent oxides selected from a group consisting of CuFeMn, CuFeAl andor CuFeAlMn multicomponent oxides.
3. The method according to claim 1, wherein the plastic surface is gasified by laser to expose the electroless plating promoter.
4. The method according to claim 3, wherein the laser has a wavelength ranging from about 157 nm to about 10.6 um with a scanning speed from about 500 to about 8000 mms, a scanning step size from about 3 to about 9 um, a scan time delay from about 30 to 100 us, a laser power from about 3 to 4 W, a frequency from about 30 to 40 KHz and a filled distance from about 10 to 50 um.
5. The method according to claim 3, wherein the electroless plating promoter is a particle with an average diameter of not greater than 100 microns.
6. The method according to claim 2, wherein the electroless plating promoter includes one or more members selected from a group consisting of
(a) Ni2O3, CO2O3, CO3O4;
(b) CuSiO3, NiSiO3, CoSiO3, CuB2O4, Cu3B2O6, NiB2O4, Ni3B2O6, NiC2O4, CoC2O4, CoC2O4;
(c) hydrogenation catalysts of Cu\u2014Zn, Cu\u2014Zn\u2014Ni, Cu\u2014Zn\u2014Co, Cu\u2014Zn\u2014Ga, Co\u2014La, Cu\u2014Cd and Cu\u2014Zn\u2014Si; and
(d) MNiO2, MMnO2, MCrO2, MAlO2, MFeO2 where M is Cu, Ni or Co.
7. The method according to claim 2, wherein the multicomponent oxides has the following formulas respectively:
CuFexMnyOz, CuFeeAlfOg and CuFeaAlbMncOd, in which x, y, z, e, f, g, a, b, c, and d satisfy: 0.1\u2266x\u22662, 0.01\u2014y\u22662, 2\u2266z\u22664; 0.01\u2266e\u22662, 0.01\u2266f\u22662, 2\u2266g\u22664; and 0.01\u2266a\u22662, 0.01\u2266b\u22662, 0.01\u2266c\u22662, 2\u2266d\u22664.
8. The method according to claim 1, wherein the supporting material is a thermoplastic material or thermosetting resin material.
9. The method according to claim 1, wherein the electroless plating promoter amounts to about 1% to about 40% of the supporting material by weight.
10. The method according to claim 8, wherein the support material further comprises at least one member selected from inorganic filler, antioxidant, light stabilizer and lubricant.
11. A method for preparing a plastic article, comprising the steps of:
1) forming at least a part of the plastic article with a support comprising a supporting material and an electroless plating promoter;
2) gasifying a surface of the support to expose the electroless plating promoter; and
3) electroless plating a layer of copper or nickel on the surface followed by electroplating or electroless plating at least one time, to form a metallized layer on the surface.
12. The method according to claim 11, wherein the electroless plating promoter in step 1) includes one or more members selected from a group consisting of:
(a) oxides of the metal elements selected from Co, Ni, Ag;
(b) silicate, borate or oxalate of metal elements selected from Co, Ni, Cu;
(c) hydrogenation catalysts having one or more metal elements selected from Cu, Zn, Ni, Co, Ga, La, Cd, Si;
(d) ABO2 type composite oxides having a delafossite structure in which A is one of metal elements selected from Co, Ni and Cu, B is an element selected from a group consisting of Ni, Mn, Cr, Al and Fe where A, B are different from each other; and
(e) multicomponent oxides selected from a group consisting of CuFeMn, CuFeAl andor CuFeAlMn multicomponent oxides.
13. The method according to claim 12, wherein the plastic article is formed by injection molding, blow molding, extruding or hot pressing.
14. The method according to claim 13, wherein the surface is gasified by laser to expose the electroless plating promoter.
15. The method according to claim 14, wherein the laser has a wavelength ranging from about 157 nm to about 10.6 um with a scanning speed from about 500 to about 8000 mms, a scanning step size from about 3 to about 9 um, a scan time delay from about 30 to 100us, a laser power from about 3 to 4 W, a frequency from about 30 to 40 KHz and a filled distance from about 10 to 50 um.
16. The method according to claim 11, wherein the step 3) further comprises performing additional electroplating orand electroless plating to form a Ni\u2014Cu\u2014Ni, Ni\u2014Cu\u2014Ni\u2014Au, Cu\u2014Ni, or Cu\u2014Ni\u2014Au layer on the support respectively.
17. The method according to claim 16, wherein the Ni layer has a thickness of about 0.1-50 um, the Cu layer has a thickness of about 0.1-100 um and the Au layer has a thickness of about 0.01-10 um respectively in the layers of Ni\u2014Cu\u2014Ni, Ni\u2014Cu\u2014Ni\u2014Au, Cu\u2014Ni and Cu\u2014Ni\u2014Au.
18. The method according to claim 11, wherein the electroless plating promoter is a particle with an average diameter of not greater than 100 microns.
19. The method according to claim 12, wherein the multicomponent oxides has the following formulas respectively: CuFexMnyOz, CuFeeAlfOg and CuFeaAlbMncOd, in which x, y, z, e, f, g, a, b, c, and d satisfy: 0.01\u2266x\u22662, 0.01\u2266y\u22662, 2\u2266z\u22664; 0.01\u2266e\u226652, 0.01\u2266f\u22662, 2\u2266g\u22664; and 0.01\u2266a\u22662, 0.01\u2266b\u22662, 0.01\u2266c\u22662, 2\u2266d\u22664.
20. The method according to claim 11, wherein the electroless plating promoter amounts to about 1% to about 40% of the support by weight.
21-24. (canceled)
The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.
1. A liquid source chemical vaporizer for vaporizing liquid source chemical and delivering vapor phase chemical, comprising:
a container configured to hold liquid source chemical up to a liquid fill level and to additionally define an inner gas volume;
a carrier gas inlet configured to communicate carrier gas into the container;
a gas outlet communicating with a vapor deposition reactor and the inner gas volume of the container; and
a porous element positioned to be in contact with liquid source chemical and in contact with the inner gas volume within the container, wherein the porous element comprises a porous gas flow divider at least partially defining a gas flow path from the carrier gas inlet to the gas outlet, wherein the gas flow divider is configured to allow vapor phase reactant to pass through while preventing liquid phase reactant from passing through.
2. The source chemical vaporizer of claim 1, wherein a porosity of the gas flow divider is selected to cause liquid chemical to migrate along the flow divider by capillary action.
3. The source chemical vaporizer of claim 2, wherein each of the carrier gas inlet and the gas outlet is arranged to open to the inner gas volume above the liquid fill level.
4. The source chemical vaporizer of claim 3, wherein the gas flow divider comprises a spiral wall extending from a bottom of the container to a ceiling of the container, wherein one of the carrier gas inlet and the gas outlet is positioned approximately at a center of the spiral and the other of the carrier gas inlet and the gas outlet is positioned approximately at an outer end of the spiral.
5. A liquid source chemical vaporizer, comprising:
an outer container configured to hold liquid source chemical;
a carrier gas inlet communicating with an inner gas volume defined within the outer container;
a gas mixture outlet communicating with a vapor deposition reactor and the inner gas volume; and
at least one flow divider defining a gas flow path through the inner gas volume, wherein the material of the at least one flow divider is microporous.
6. The source chemical vaporizer of claim 5, wherein the at least one flow divider comprises a material selected for causing liquid chemical to wet the flow divider by capillary action.
7. The source chemical vaporizer of claim 5, wherein the flow divider extends a height of the outer container from an outer container floor to an outer container ceiling.
8. The source chemical vaporizer of claim 7, wherein the flow divider has a spiral shape, and one of the gas inlet and gas outlet communicates with the inner gas volume overlying liquid source chemical proximate a center of the spiral, while the other of the gas inlet and the gas outlet communicates with the inner gas volume proximate an outer edge of the spiral flow divider.
9. The source chemical vaporizer of claim 5, wherein the material of the at least one flow divider has a porosity between about 30% and 70%.
10. The source chemical vaporizer of claim 5, wherein the at least one flow divider comprises a semi-porous, breathable membrane in contact with each of the gas flow path and the liquid source chemical.
11. The source chemical vaporizer of claim 5, wherein the material of the at least one flow divider has a porosity between about 20% and 80%.
12. The source chemical vaporizer of claim 5, wherein the material of the at least one flow divider is absorbent.
13. The source chemical vaporizer of claim 5, wherein a nominal radius of pores in the microporous material is between about 10 \u03bcm and 200 \u03bcm.
14. The source chemical vaporizer of claim 5, wherein a nominal radius of pores in the microporous material is between about 30 \u03bcm and 70 \u03bcm.
15. The source chemical vaporizer of claim 8, wherein distance of a gas flow path between the gas inlet to the gas outlet is about 3 times greater than a linear distance between the gas inlet and the gas outlet.
16. The source chemical vaporizer of claim 8, wherein distance of a gas flow path between the gas inlet to the gas outlet is about 5 times greater than a linear distance between the gas inlet and the gas outlet.