What is claimed is:
1. A method for manufacturing galvanized steel sheet, comprising the step of adjusting a surface texture of a galvanized steel sheet by blasting solid particles against a surface of the galvanized steel sheet.
2. The method according to claim 1, wherein the surface texture is at least one selected from the group consisting of an mean roughness Ra on the surface of the steel sheet, a peak count PPI on the surface of the steel sheet, and a filtered centerline waviness Wca on the surface of the steel sheet.
3. The method according to claim 1, wherein the step of adjusting the surface texture comprises adjusting the mean roughness Ra on the surface of the steel sheet to a range of from 0.3 to 3 m.
4. The method according to claim 1, wherein the step of adjusting the surface texture comprises adjusting the peak count PPI on the surface of the steel sheet to 250 or more.
5. The method according to claim 1, wherein the step of adjusting the surface texture comprises adjusting the filtered centerline waviness Wca on the surface of the steel sheet to 0.8 m or less.
6. The method according to claim 1, wherein the solid particles have average particle sizes of from 10 to 300 m.
7. The method according to claim 1, wherein the solid particles are metallic particles.
8. The method according to claim 1, wherein the solid particles are in near-spherical shape.
9. The method according to claim 1, wherein the step of adjusting the surface texture comprises adjusting the surface texture of the galvanized steel sheet by blasting solid particles against the surface of the galvanized steel sheet at blasting speeds of from 30 to 300 msec.
10. The method according to claim 1, wherein the step of adjusting the surface texture comprises adjusting the surface texture of the galvanized steel sheet by blasting solid particles against the surface of the galvanized steel sheet at blasting densities of from 0.2 to 40 kgm2.
11. The method according to claim 1, wherein the galvanized steel sheet has a coating film consisting essentially of phase.
12. The method according to claim 1, further comprising the step, before the step for adjusting the surface texture, of temper rolling to the galvanized steel sheet to adjust the filtered centerline waviness Wca to 0.7 m or less.
13. The method according to claim 1, wherein the step of adjusting the surface texture comprises blasting solid particles having average particle sizes of from 30 to 300 m against the surface of the galvanized steel sheet, using a wheel blast machine having a distance of 700 mm or less between a rotational center of a wheel thereof and a steel strip.
14. The method according to claim 13, wherein the solid particles have 85% or more weight percentage of the solid particles having size thereof within a range of from 0.5d to 2d to the total weight of the solid particles, where d designates the mean particle size.
15. The method according to claim 13, wherein the solid particles have density of 2 gcm3 or more.
16. A galvanized steel sheet having a dimple-pattern surface.
17. A galvanized steel sheet having a dimple-pattern surface, which is manufactured by the method according to claim 1.
18. The galvanized steel sheet according to claim 16, wherein the surface has mean roughness Ra ranging from 0.3 to 3 m.
19. The galvanized steel sheet according to claim 16, wherein the surface has peak counts PPI expressed by the formula:
50Ra(m)300<PPI<600
20. The galvanized steel sheet according to claim 16, wherein the surface has peak count PPI of at least 250.
21. The galvanized steel sheet according to claim 16, wherein the surface has filtered centerline waviness Wca of 0.8 m or less.
22. The galvanized steel sheet according to claim 16, wherein the galvanized steel sheet has a coating film consisting essentially of phase.
23. The galvanized steel sheet according to claim 16, wherein the galvanized steel sheet has number densities of concavities of 3.1102 countsmm2 or more at a depth level corresponding to 80% bearing area ratio.
24. The galvanized steel sheet according to claim 16, wherein the surface has a texture giving core fluid holding indexes Sci of 1.2 or more.
25. The galvanized steel sheet according to claim 16, further comprising a solid lubrication film having average thickness ranging from 0.001 to 2 m on the surface of the galvanized steel sheet, the solid lubrication film being at least one film selected from the group consisting of an inorganic solid lubrication film, an organic solid lubrication film, and an organic-inorganic composite solid lubrication film.
26. The galvanized steel sheet according to claim 25, wherein the solid lubrication film is a phosphorus-base oxide film obtained by applying and drying an aqueous solution containing phosphoric acid and at least one cationic component selected from the group consisting of Fe, Al, Mn, Ni, and NH4.
27. The galvanized steel sheet according to claim 26, wherein
the solid lubrication film contains a P component and an N component, and at least one component selected from the group consisting of Fe, Al, Mn, and Ni;
the solid lubrication film has a molar ratio (a)(b) in a range of from 0.2 to 6, where (b) designates the amount of P component, and (a) designates the total amount of N component, Fe, Al, Mn, and Ni;
the amount of P component is expressed by a P2O5 converted value, and the amount of N component is expressed by an ammonium converted value.
28. The galvanized steel sheet according to claim 26, wherein the solid lubrication film contains the P component and the N component as the solid lubrication film components in a form of chemical compound selected from the group consisting of a nitrogen compound, a phosphorus-base compound, and a nitrogen-phosphorus-base compound.
29. The galvanized steel sheet according to claim 26, wherein the solid lubrication film contains at least Fe as the solid lubrication film component.
30. A method for manufacturing galvanized steel sheet of claim 26, comprising the steps of:
applying an aqueous solution containing a cationic component () and a phosphoric acid component () on the surface of plated layer of a galvanized steel sheet, and drying the applied film without washing thereof with water, thus forming a coating film;
wherein the cationic component () consists essentially of at least one metallic ion or cation selected from the group consisting of Mg, Al, Ca, Ti, Fe, Co, Ni, Cu, Mo, and NH4; and
the aqueous solution has a molar concentration ratio ()() ranging from 0.2 to 6, where () designates the total amount of cations, and () designates the amount of phosphoric acid component; the phosphoric acid is expressed by the value converted to P2O5 molar concentration.
31. A method for manufacturing press-formed product, comprising:
the first step of preparing a galvanized steel sheet member having a dimple-pattern surface; and
the second step of applying press-forming to the member to obtain designed shape of press-formed product.
32. The method according to claim 31, wherein the surface has mean roughness Ra ranging from 0.3 to 3 m.
33. The method according to claim 31, wherein the surface has peak count PPI expressed by the formula:
50Ra(m)300<PPI<600
34. The method according to claim 31, wherein the surface has peak count PPI of at least 250.
35. The method according to claim 31, wherein the surface has filtered centerline waviness Wca of 0.8 m or less.
The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.
1. An ink jet recording material comprising a support and at least one binder containing ink-receiving layer, characterized in that said at least one ink-receiving layer further contains a compound according to following general formula (I):
A-L-R\u2003\u2003(I)
wherein,
A is represented by following formula:
\u2003wherein:
Z represents the necessary atoms to complete a five- or six-membered ring,
R1 to R4 independently represent a substituted or unsubstituted C1 to C6 aliphatic group,
X is selected from the group consisting of a hydrogen, a substituted or unsubstituted aliphatic group, an acyl group, an oxy radical, a hydroxyl group, an alkoxy group an \u2014OSO2-alkyl group, and an acyloxy group;
L is a divalent linking group, linked to the five- or six-membered ring by one of the atoms of Z, optionally by a double bond, wherein said divalent linking group comprises a nitrogen-nitrogen or nitrogen-oxygen bond,
\u2014R represents a non aromatic moiety comprising at least two hydroxyl groups.
2. Ink-jet recording material according to claim 1, wherein said recording material further comprises a pigment in at least one ink-receiving layer.
3. Ink-jet recording material according to claim 2 wherein said pigment is an inorganic pigment.
4. Ink-jet recording material according to claim 3 wherein said inorganic pigment is chosen from the group consisting of silica, alumina, aluminum silicate, and aluminum trihydroxide.
5. An ink jet recording material comprising a support and at least one binder containing ink-receiving layer, characterized in that said at least one ink-receiving layer further contains a compound according to following general formula (II):
wherein,
R1 to R4 independently represent a substituted or unsubstituted C1 to C6 aliphatic group,
X is selected from the group consisting of a hydrogen, a substituted or unsubstituted aliphatic group, an acyl group, an oxy radical, a hydroxyl group, an alkoxy group an \u2014OSO2-alkyl group, and an acyloxy group,
L is a divalent linking group, linked to the six-membered ring optionally by a double bond, wherein said divalent linking group comprises a nitrogen-nitrogen or nitrogen-oxygen bond,
R represents a non aromatic moiety comprising at least two hydroxyl groups.
6. An ink jet recording material according to claim 5, wherein said compound is represented by following formula (V):
wherein,
R1 to R4 independently represent a substituted or unsubstituted C1 to C6 aliphatic group,
X is selected from the group consisting of a hydrogen, a substituted or unsubstituted aliphatic group, an acyl group, an oxy radical, a hydroxyl group, an alkoxy group an \u2014OSO2-alkyl group, and an acyloxy group,
Y represents an oxygen or NR5; R5 is selected from the group consisting of a hydrogen, a substituted or unsubstituted, saturated or unsaturated aliphatic group, a substituted or unsubstituted aromatic group, a substituted or unsubstituted hetero-aromatic group, and an acyl group; and
R represents a non-aromatic moiety comprising at least two hydroxyl groups.