1. A sealing material for use in a solar cell module, comprising: a monolayer or multilayer film comprising a resin composition containing at least 90 mass % of a polyethylene-based resin with a density of at most 0.900 gcm3 and containing substantially no crosslinking coagent,
the monolayer or multilayer film having a MFR of from 0.1 g10 min to 1.0 g10 min as measured at 190\xb0 C. under a load of 2.16 kg according to JIS K 7210.
2. The sealing material according to claim 1, wherein the polyethylene-based resin is metallocene-type linear low density polyethylene.
3. The sealing material according to claim 1, wherein the polyethylene-based resin contains a copolymer obtained by copolymerization using an \u03b1-olefin and an ethylenic unsaturated silane compound as comonomers.
4. The sealing material according to claim 1, which has a gel fraction of at most 25%.
5. The sealing material according to claim 1, which has a polystyrene-equivalent weight average molecular weight of from 120,000 to 300,000.
6. The sealing material according to claim 1, which has at least two layers different in the MFR.
7. The sealing material according to claim 6, wherein the layers include a layer with a relatively high MFR arranged as an outermost layer and another layer with a relatively low MFR arranged as an intermediate layer.
8. A solar cell module having the sealing material according to claim 1.
9. A method for producing a sealing material for use in a solar cell module, comprising: melt molding a resin composition containing a polyethylene-based resin with a density of at most 0.900 gcm3 and 0.02 mass % to less than 0.5 mass % of a polymerization initiator.
10. The method for producing a sealing material for use in a solar cell module according to claim 9, wherein the composition contains 0.02 mass % to 0.2 mass % of the polymerization initiator.
11. The method for producing a sealing material for use in a solar cell module according to claim 9, wherein the polymerization initiator is an organic peroxide.
12. The method for producing a sealing material for use in a solar cell module according to claim 9, wherein the melt molding is performed at a temperature at least 50\xb0 C. higher than the melting point of the polyethylene-based resin.
13. The method for producing a sealing material for use in a solar cell module according to claim 9, wherein a difference in the density of the resin composition between before and after the melt molding is at most 0.05 gcm3, and
a difference in the MFR of the resin composition between before and after the melt molding is at least 1.0 g10 min as measured at 190\xb0 C. under a load of 2.16 kg according to JIS K 7210.
14. The method for producing a sealing material for use in a solar cell module according to claim 9, wherein the sealing material has at least two layers different in polymerization initiator content.
15. The method for producing a sealing material for use in a solar cell module according to claim 14, wherein the layers include a layer with a relatively low polymerization initiator content arranged as an outermost layer and another layer with a relatively high polymerization initiator content arranged as an intermediate layer.
16. The sealing material according to claim 2, wherein the polyethylene-based resin contains a copolymer obtained by copolymerization using an \u03b1-olefin and an ethylenic unsaturated silane compound as comonomers.
17. The sealing material according to claim 3, which has a gel fraction of at most 25%.
18. The sealing material according to claim 4, which has a polystyrene-equivalent weight average molecular weight of from 120,000 to 300,000.
19. The sealing material according to claim 5, which has at least two layers different in the MFR.
20. The sealing material according to claim 3, which has at least two layers different in the MFR.
The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.
1. A process for making ZIF membranes comprising:
exposing a support material to a ZIF synthesis solution comprising metal ions or metal clusters, and imidazolate under conditions suitable for ZIF crystal formation; and
forming a ZIF membrane having a thickness in a range from about 1 micron to about 100 microns and a pore size in a range from 0.2 nm to about 0.5 nm.
2. The process of claim 1 wherein the membrane material is a ZIF material with pore size from 0.3 nm to 0.4 nm.
3. The process of claim 2 wherein the ZIF material is ZIF-8, ZIF-67, ZIF-7 or ZIF-65.
4. The process of claim 3 wherein the ZIF materials is ZIF-8 and ZIF-67.
5. The process of claim 4 wherein the membrane is synthesized in aqueous solution.
6. The process of claim 4 wherein the membrane is synthesized at a temperature between 10 to 100\xb0 C.
7. The process of claim 1 wherein the support material is alpha-alumina, stainless steel, nickel, glass or polymer.
8. The process of claim 1 wherein the support material is flat-sheet, tube, hollow fiber or monolith.
9. A method to separate mixtures of C2\u2212 and C3+ components, comprising
providing a stream containing at least one component of C2\u2212 and at least one component of C3+ in different composition ratios;
providing a ZIF membrane comprising a plurality of porous ZIF grains that form a ZIF layer supported on a support materials, wherein the ZIF layer has a thickness in the range from 1 micron to 100 micron and a pore size in the range from 0.2 nm to 0.5 nm; and
performing a membrane separation process by feeding the stream to be separated to the feed side of the membrane such that C2\u2212 hydrocarbon will pass preferentially through the membrane thereby providing a permeate stream enriched in C2\u2212 hydrocarbons and a retentate enriched in C3+ hydrocarbon.
10. The method of claim 9, wherein the C2\u2212 component is hydrogen, nitrogen, oxygen, methane ethane or ethanol.
11. The method of claim 9, wherein the C3+ component is propane, propylene, butane, butylenes, isobutene, propanol, isopropanol or butanol.
12. A method as in claim 9, wherein the support material is alpha-alumina, stainless steel, nickel, glass or polymer.
13. A method as in claim 9, wherein the support material is flat-sheet, tube, hollow fiber or monolith.
14. A method as in claim 9, wherein the driving force for the membrane separation process is provided either by applying pressure on the feed side or by drawing a vacuum on the permeate side.
15. A process as in claim 9, where a mixture of hydrogen and propane can be separated with separation factor of at least 40, with permeance of hydrogen greater than 2000\xd710\u221210 molm2 s Pa.
16. A process as in claim 9, where a mixture of hydrogen and propylene can be separated with separation factor of at least 10, with permeance of hydrogen greater than 2000\xd710\u221210 molm2 s Pa.
17. A process as in claim 9, where a mixture of ethane and propane can be separated with separation factor of at least 40, with permeance of ethane greater than 500\xd710\u221210 molm2 s Pa.
18. A process as in claim 9, where a mixture of ethylene and propylene can be separated with separation factor of at least 5, with permeance of ethylene greater than 1000\xd710\u221210 molm2 s Pa.
19. A process as in claim 9, where a mixture of ethylene and propane can be separated with separation factor of at least 40, with permeance of ethylene greater than 800\xd710\u221210 molm2 s Pa.
20. A process as in claim 9, where a mixture of ethanol and isopropanol can be separated with separation factor of at least 500, with permeance of ethanol greater than 8\xd710\u22128 molm2 s Pa.
21. A method to separate mixtures of propylene and propane components, comprising
providing a stream containing a propylene component and a propane component;
providing a ZIF membrane comprising a plurality of porous ZIF grains that form a ZIF layer supported on a support materials, wherein the ZIF layer has a thickness in the range from 1 micron to 100 micron and a pore size in the range from 0.2 nm to 0.5 nm; and
performing a membrane separation process by feeding the stream to be separated to the feed side of the membrane such that propylene will pass preferentially through the membrane thereby providing a permeate stream enriched in propylene and a retentate enriched in propane.
22. A process as in claim 9, where a mixture of propylene and propane can be separated with a separation factor of at least 25, with permeance of propylene greater than 2\xd710\u22128 molm2 s Pa.
23. The process of claim 1, further comprising depositing a plurality of ZIF seed particles having a pore size from about 0.2 nm to about 0.5 nm on a support forming a ZIF seed layer prior to exposing the support to the ZIF synthesis solution.