What is claimed is:
1. A method of forming a silicon nitride deposited film using the capacitive coupled plasma enhanced CVD process, which comprises disposing a plate high-frequency electrode for supplying a high-frequency power of the VHF band and a grounding electrode in opposition to each other at an interval of less than 8 mm in a vacuum vessel, introducing at least a silane-based gas and nitrogen gas as source gases into a reaction space of the vacuum vessel, and forming a silicon nitride deposited film with the pressure of the reaction space being kept at 40 to 133 Pa.
2. The method according to claim 1, wherein a density of a power supplied to the high-frequency electrode is 40 to 150 mWcm2.
3. The method according to claim 2, wherein the flow rate of the nitrogen gas is 10 to 30 times that of the silane-based gas.
4. The method according to claim 1, wherein the temperature of a substrate on which the silicon nitride film is deposited is 80 C. or less.
5. The method according to claim 1, wherein the silicon nitride film is formed on another deposited film comprising an organic film.
6. A method of producing an organic electroluminescent device having an organic electroluminescent element provided on a substrate, comprising:
the element forming step of forming on a substrate an organic electroluminescent element comprising a pair of electrodes and an organic material interposed between the pair of electrodes; and
the silicon nitride film forming step, subsequently to the element forming step, of forming a silicon nitride film so as to cover the organic electroluminescent element,
wherein the silicon nitride film forming step comprises disposing a plate high-frequency electrode for supplying a high-frequency power of the VHF band and a grounding electrode in opposition to each other at an interval of less than 8 mm in a vacuum vessel, introducing at least a silane-based gas and nitrogen gas as source gases into a reaction space of the vacuum vessel, and forming a silicon nitride film with the pressure of the reaction space being kept at 40 to 133 Pa.
7. The method according to claim 6, wherein of the pair of electrodes of the electroluminescent element, the electrode on the substrate side is a reflecting electrode and the other electrode is a transparent electrode.
8. The method according to claim 7, wherein the silicon nitride film covers not only the transparent electrode but also a side portion of the organic electroluminescent element.
The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.
1. An integrated battery comprising
(a) a flexible substrate and
(b) at least one cell group comprising 4 unit cells arranged on said flexible substrate;
each of said unit cells comprising a positive electrode, a negative electrode and a solid electrolyte interposed between said positive electrode and said negative electrode, and
said cell group having a shape of a rectangle and having strip-shaped plain portions arranged along 2 diagonal lines of said rectangle, said plain portions dividing said rectangular cell group into said 4 unit cells.
2. The integrated battery in accordance with claim 1, wherein said strip-shaped plain portions have a width twice or more times larger than the thickness of said unit cell.
3. The integrated battery in accordance with claim 1, wherein said flexible substrate has a rectangular outer shape, said outer shape being geometrically similar to said shape of said cell group, and said cell group is arranged on said flexible substrate such that each side of said flexible substrate and the corresponding side of said cell group are parallel.