1461083265-883b4f34-4b76-459c-b0b6-2a614913e903

1: A fire retardant thermoplastic resin composition comprising a matrix resin that comprises 20 to 35% by weight of a poly arylene ether resin, 20 to 35% by weight of a vinyl aromatic resin and 5 to 20% by weight of an olefin-based resin, 1 to 10% by weight of a room-temperature liquid-type fire retardant, and 8 to 20% by weight of an ancillary fire retardant, based on 100% by weight of a mixture of a poly arylene ether resin, a vinyl aromatic resin, an olefin-based resin, a room-temperature liquid-type fire retardant and an ancillary fire retardant.
2: The fire retardant thermoplastic resin composition according to claim 1, wherein the olefin-based resin is selected from the group consisting of low-density polyethylene (LDPE), high-density polyethylene (HDPE), polypropylene and mixtures of two or more thereof.
3: The fire retardant thermoplastic resin composition according to claim 1, wherein the room-temperature liquid-type fire retardant is a room-temperature liquid-type phosphorus-based fire retardant.
4: The fire retardant thermoplastic resin composition according to claim 1, wherein the room-temperature liquid-type fire retardant is comprised in an amount of 3 to 8% by weight.
5: The fire retardant thermoplastic resin composition according to claim 3, wherein the room-temperature liquid-type phosphorus-based fire retardant is selected from the group consisting of bisphenol-A-diphenyl phosphate (BPADP), triphenyl phosphate (TPP), resorcinol bis-diphenyl phosphate (RDP) and mixtures of two or more thereof.
6: The fire retardant thermoplastic resin composition according to claim 1, wherein the ancillary fire retardant comprises 7 to 15% by weight of a nitrogen-based fire retardant.
7: The fire retardant thermoplastic resin composition according to claim 6, wherein the nitrogen-based fire retardant is one or more selected from the group consisting of melamine polyphosphate, melamine pyrophosphate and melamine phosphate.
8: The fire retardant thermoplastic resin composition according to claim 6, wherein the ancillary fire retardant further comprises 1 to 5% by weight of a second phosphorus-based fire retardant other than the room-temperature liquid-type phosphorus-based fire retardant.
9: The fire retardant thermoplastic resin composition according to claim 8, wherein the second phosphorus-based fire retardant is one or more selected from the group consisting of metal phosphate, a phosphorus ester compound, phosphate, pyrophosphate, phosphonate, metal-substituted phosphinate and phosphanate.
10: The fire retardant thermoplastic resin composition according to claim 9, wherein the metal phosphate is aluminium phosphate, zinc phosphate or a mixture thereof.
11: The fire retardant thermoplastic resin composition according to claim 1, wherein a melt index of the fire retardant thermoplastic resin composition is 40 to 150 g10 min.
12: An electric wire comprising the fire retardant thermoplastic resin composition according to claim 1.

The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.

1. A method of producing steel for a steel pipe excellent in sour-resistance performance, wherein the steel comprises, in % by mass, C: 0.03 to 0.4%, Mn: 0.1 to 2%, Si: 0.01 to 1%, P: 0.015% or less, S: 0.002% or less, Ti: 0.2% or less, Al: 0.005 to 0.1%, Ca: 0.0005 to 0.0035%, N: 0.01% or less, and O (oxygen): 0.002% or less, the balance being Fe and impurities, the method comprising controlling the amount of Ca addition charged into the steel that is molten in a ladle according to a N content in the molten steel prior to Ca addition, wherein non-metallic inclusions in the steel are mainly composed of Ca, Al, O and S, and, as a result of the controlling step, a CaO content in the inclusions is in the range of 30 to 80%, the ratio of the N content in the steel to the CaO content in the inclusions satisfies the relation expressed by equation (1), and a CaS content in the inclusions satisfies the relation expressed by equation (2),
0.28\u2266N(% CaO)\u22662.0\u2003\u2003(1)
(% CaS)\u226625%\u2003\u2003(2)

where N represents the mass content (ppm) of N in the steel, (% CaO) represents the mass content (%) of CaO in the inclusions, and (% CaS) represents the mass content (%) of CaS in the inclusions,
the steel comprising one or more compositional elements in place of a part of Fe selected from the group constisting of (a), (b), and (c) below:
(a) in % by mass, Cr: 1% or less, Mo: 1% or less, Nb: 0.1% or less, and V: 0.3% or less;
(b) in % by mass, Ni: 0.3% or less, and Cu: 0.4% or less; and
(c) in % by mass, B: 0.002% or less.
2. The method of producing steel for a steel pipe excellent in sour-resistance performance according to claim 1, wherein Ca is added such that in controlling the amount of Ca addition into the molten steel in the ladle, the ratio of the N content in molten steel to the amount of Ca addition to the molten steel satisfies the relation expressed by equation (3) below according to the N content in the molten steel prior to the Ca addition:
200\u2266NWCA\u2266857\u2003\u2003(3)

where N represents the mass content (ppm) of N in the molten steel prior to the Ca addition and WCA represents the amount of Ca addition (kgt-molten steel) to the molten steel.
3. The method of producing steel for a steel pipe excellent in sour-resistance performance according to claim 2,
wherein the molten steel is treated by the steps indicated by Steps 1 to 4 and then the Ca is added in Step 5:
Step 1: CaO-type flux is added to molten steel in a ladle at atmospheric pressure;
Step 2: after Step 1, the molten steel and the CaO flux are stirred by injecting a stirring gas into the molten steel in the ladle at atmospheric pressure, and also an oxidizing gas is supplied to the molten steel to thereby mix the CaO-type flux with an oxide generated by the reaction of the oxidizing gas with the molten steel;
Step 3: the supply of the oxidizing gas is halted and desulfurization and removal of inclusions are carried out by injecting a stirring gas into the molten steel in the ladle at atmospheric pressure;
Step 4: an oxidizing gas is supplied into an Ruhrstahl-Heraeus(RH) vacuum chamber to increase the molten steel temperature when the molten steel in the ladle is treated using an RH degasser after Step 3, and subsequently the supply of the oxidizing gas is halted, and then circulation of the molten steel within the RH degasser is continued to remove inclusions in the molten steel; and
Step 5: metallic Ca or a Ca alloy is added to the molten steel in the ladle after Step 4.
4. The method of producing steel for a steel pipe excellent in sour-resistance performance according to claim 1,
wherein the molten steel is treated by the steps indicated by Steps 1 to 4 and then the Ca is added in Step 5:
Step 1: CaO-type flux is added to molten steel in a ladle at atmospheric pressure;
Step 2: after Step 1, the molten steel and the CaO flux are stirred by injecting a stirring gas into the molten steel in the ladle at atmospheric pressure, and also an oxidizing gas is supplied to the molten steel to thereby mix the CaO-type flux with an oxide generated by the reaction of the oxidizing gas with the molten steel;
Step 3: the supply of the oxidizing gas is halted and desulfurization and removal of inclusions are carried out by injecting a stirring gas into the molten steel in the ladle at atmospheric pressure;
Step 4: an oxidizing gas is supplied into an Ruhrstahl-Heraeus(RH) vacuum chamber to increase the molten steel temperature when the molten steel in the ladle is treated using an RH degasser after Step 3, and subsequently the supply of the oxidizing gas is halted, and then circulation of the molten steel within the RH degasser is continued to remove inclusions in the molten steel; and
Step 5: metallic Ca or a Ca alloy is added to the molten steel in the ladle after Step 4.