1461087521-e9f3eb3b-2be4-43d1-9f99-39f7035d3bcd

1. A transceiver module usable in fiber-optic communication applications, the transceiver module comprising:
a receiver optical subassembly configured to receive optical signals;
a transmitter optical subassembly configured to transmit optical signals;
a connector adapted to couple the transceiver to an IC voltage associated with an external power supply;
a voltage filter adapted to receive the IC voltage from the external power supply and generate a filtered voltage at a voltage level less than the IC voltage; and
a signal processing integrated circuit powered by the filtered voltage, the signal processing integrated circuit designed to be operated at the voltage level of the filtered voltage.
2. The transceiver module of claim 1, further comprising an LC filter coupled to the voltage filter.
3. The transceiver module of claim 1, wherein the signal processing integrated circuit is a clock and data recovery circuit.
4. The transceiver module of claim 1, wherein the signal processing integrated circuit is an eye-opening circuit.
5. The transceiver module of claim 1, wherein the voltage filter is a low-dropout linear filter.
6. The transceiver module of claim 1, wherein the voltage filter is a passive filter.
7. The transceiver module of claim 1, wherein the voltage filter is an active filter.
8. The transceiver module of claim 1, wherein the voltage filter is adapted to filter harmful noise in the range from about 10 Khz to about 3 Mhz.
9. The transceiver module of claim 1, wherein the at least one IC voltage is at least one of 1.8V, 3.3V and 5 V.
10. The transceiver module of claim 1, wherein the signal processing integrated circuit is an application specific integrated circuit.

The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.

We claim:

1. A film layer prepared by a melt extrusion process, the film layer having a thickness of from 3 to 75 microns, a molecular weight distribution of from 2 to 4, a machine direction tensile strength of from 50 MPa to 120 MPa and a transverse direction tensile strength higher than 45 MPa.
2. The film layer of claim 1, wherein the film layer has a thickness of from 3 to 75 microns, a molecular weight distribution of from 2 to 4, a machine direction tensile strength of from 55 MPa to 100 MPa and a transverse direction tensile strength higher than 45 MPa.
3. The film layer of claim 1, wherein the melt extrusion process is a melt extrusion of a thermoplastic olefin having at least 80% by weight of ethylene derived units, a melt index of from 0.2 to 8, and a melt index ratio of less than 30.
4. The film layer of claim 1, wherein the film layer has a density of from 0.910 to 0.935 gcm3 and a transverse Elemendorf tear strength greater than 500 gmil.
5. A film layer prepared by a process comprising:
(a) selecting a thermoplastic polyolefin having a characteristic time (c) determined by fitting a curve of dynamic viscosity (*) vs. frequency of oscillation () such that
*()01(c)m,
where 0 is the zero shear viscosity and m is a power law index, and said c is a value of from 0.001 to 0.6 s;
(b) setting the aspect ratio (A) of the air gap length (X) to one-half an extrusion die orifice width (L0) to lower than 0.8, where X is defined as the distance from said die orifice of a melt extruder to the location on a chill roll where extrudate of said polyolefin is solidified;
(c) extruding the film through said extrusion die orifice onto said chill roll while maintaining a ratio (Dr) of film velocity at said chill roll (uf) to film velocity at said die orifice (uo) of at least 30; and
(d) maintaining the product (De) of said c times the ratio of said film velocity at the die orifice (u0) to said air gap length (X) at a value greater than 0.005.
6. The film layer of claim 5, wherein the film layer has a thickness of from 3 to 75 microns, a molecular weight distribution of from 2 to 4, a machine direction tensile strength of from 50 MPa to 120 MPa and a transverse direction tensile strength higher than 45 MPa.
7. The film layer of claim 5, wherein the film layer has a thickness of from 3 to 75 microns, a molecular weight distribution of from 2 to 4, a machine direction tensile strength of from 55 MPa to 100 MPa and a transverse direction tensile strength higher than 45 MPa.