1461092315-49e2dddb-9827-489a-800a-9aebeba10b0a

1. A process for producing an oxygen-absorbing package, which comprises:
(a) producing an oxygen-absorbing composition comprising a granular iron powder as an effective component which contains fine iron powder passing through a 200-mesh standard sieve in an amount of 5% by weight or less by removing the fine iron powder; and
(b) packaging the oxygen-absorbing composition in an air-permeable packaging material using a three-sided automatic filling-packaging machine of rotary filling type in a high productivity of at least several hundred packages per minute, wherein amount of the iron powder attached to an outer surface of the oxygen-absorbing package is 0.5 mgm2 or less with respect to a surface area of the oxygen-absorbing package.
2. The process according to claim 1, wherein the iron powder is a sponge iron powder.
3. The process according to claim 1, wherein the granular iron powder is a coated iron powder prepared by coating an iron powder with an electrolyte in an amount of 0.1 to 10% by weight based on the weight of the iron powder.
4. The process according to claim 3, wherein said coated iron powder is produced by first coating iron powder and then removing the fine iron powder.
5. The process according to claim 3, wherein said coated iron powder is produced by first removing fine iron powder, leaving remaining iron powder, and then coating the remaining iron powder.
6. The process according to claim 5, wherein said coated iron powder is produced by further removing fine iron powder again, after the coating.
7. The process according to claim 1, wherein the removal of the fine iron powder is conducted by screening or separation method utilizing gravity or centrifugal force.
8. The process according to claim 1, wherein said granular iron powder contains fine iron powder passing through a 200-mesh standard sieve in an amount of 3% by weight or less.
9. The process according to claim 1, wherein average particle size of the granular iron powder is 100 to 250 \u03bcm.
10. The process according to claim 1, wherein the granular iron powder includes at most 3% by weight coarse iron powder having a diameter larger than 500 \u03bcm.
11. The process according to claim 1, wherein said high productivity of said three-sided automatic filling-packaging machine of rotary filling type is in a range of several hundred packages up to 1000 packages per minute.
12. The process according to claim 11, wherein said high productivity is in a range of 400-1000 packages per minute.
13. The process according to claim 1, in which said packaging is performed, using said three-sided automatic filling-packaging machine, by bag-making, metering and filling operations performed arranged around an axis of rotation.
14. The process according to claim 13, wherein said high productivity of said three-sided automatic filling-packaging machine of rotary filling type is in a range of several hundred packages up to 1000 packages per minute.
15. The process according to claim 14, wherein said high productivity is in a range of 400-1000 packages per minute.

The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.

1. A high capacity, high charge rate lithium secondary cell, comprising:
a high capacity lithium-containing positive electrode in electronic contact with a positive electrode current collector, the current collector in electrical connection with an external circuit;
a high capacity negative electrode in electronic contact with a negative electrode current collector, said current collector in electrical connection with an external circuit;
a separator positioned between and in ionic contact with the cathode and the anode; and
an electrolyte in ionic contact with the positive and negative electrodes,
wherein the total area specific impedance for the cell and the relative area specific impedances for the positive and negative electrodes are such that, during charging at greater than or equal to 4C, the negative electrode potential is above the potential of metallic lithium.
2. A high capacity, high charge rate lithium secondary cell, comprising:
a lithium-containing positive electrode in electronic contact with a positive electrode current collector, said current collector in electrical connection with an external circuit;
a negative electrode in electronic contact with a negative electrode current collector, said current collector in electrical connection with an external circuit;
a separator positioned between and in ionic contact with the cathode and the anode; and
an electrolyte in ionic contact with the positive and negative electrodes,
wherein the charge capacity per unit area of the positive and negative electrodes each are at least 0.75 mA-hcm2, and
wherein the total area specific impedance for the cell is less than about 20 \u03a9-cm2.
3. The lithium secondary cell of claim 1, wherein the area specific impedance of the total cell is localized predominantly at the positive electrode.
4. The lithium secondary cell of claim 1, wherein the charge capacity per unit area of the positive and negative electrodes each are at least 0.75 mA-hcm2.
5. The lithium secondary cell of claim 1 or 2, wherein the current capacity per unit area of the positive and negative electrodes each are at least 1.0 mA-hcm2.
6. The lithium secondary cell of claim 1 or 2, wherein the charge capacity per unit area of the positive and negative electrodes each are at least 1.5 mA-hcm2.
7. The lithium secondary batter of claim 1, wherein the total area specific impedance for the cell is less than about 20 \u03a9-cm2, and wherein the positive electrode has an area specific impedance r1 and the negative electrode has an area specific impedance r2, and wherein the ratio of r1 to r2 is at least about 10.
8. The lithium secondary cell of claim 7, wherein the total area specific impedance for the cell is less than about 16 \u03a9-cm2 and wherein the ratio of r1 to r2 is at least about 7.
9. The lithium secondary cell of claim 7, wherein the total area specific impedance for the cell is less than about 14 \u03a9-cm2 and wherein the ratio of r1 to r2 is at least about 6.
10. The lithium secondary cell of claim 7, wherein the total area specific impedance for the cell is less than about 12 \u03a9-cm2 and wherein the ratio of r1 to r2 is at least about 5.
11. The lithium secondary cell of claim 7, wherein the total area specific impedance for the cell is less than about 10 \u03a9-cm2 and wherein the ratio of r1 to r2 is at least about 4.
12. The lithium secondary cell of claim 7, wherein the total area specific impedance for the cell is less than about 8 \u03a9-cm and wherein the ratio of r1 to r2 is at least about 3.
13. The lithium secondary cell of claim 7, wherein the current capacity per unit area of the positive and negative electrodes each are at least 1.5 mA-hcm2.
14. The lithium cell of claim 2, wherein the total area specific impedance for the cell is less than about 16 \u03a9-cm2.
15. The lithium cell of claim 2, wherein the total area specific impedance for the cell is less than about 14 \u03a9-cm2.
16. The lithium cell of claim 2, wherein the total area specific impedance for the cell is less than about 12 \u03a9-cm2.
17. The lithium cell of claim 2, wherein the total area specific impedance for the cell is less than about 10 \u03a9-cm2.
18. The lithium secondary cell of claim 2, wherein the negative electrode has an area specific impedance, r2, of less than or equal to about 3.0 \u03a9-cm2.
19. The lithium secondary cell of claim 2, wherein the negative electrode has an area specific impedance, r2, of less than or equal to about 2.5 \u03a9-cm2.
20. The lithium secondary cell of claim 2, wherein the negative electrode has an area specific impedance, r2, of less than or equal to about 2.0 \u03a9-cm2.
21. The lithium secondary cell of claim 2, wherein the negative electrode has an area specific impedance, r2, of less than or equal to about 1.5 \u03a9-cm2.
22. The lithium secondary cell of claim 1 or 2, wherein the positive electrode has a charge and discharge capacity measured at a C-rate of 10C that is greater than 90% of the nominal capacity measured at a C-rate of 110C.
23. The lithium secondary cell of claim 1 or 2, wherein the conductivity of the positive electrode does not increase more than a factor of 2 over the state of charge.
24. The lithium secondary cell of claim 1 or 2, wherein the conductivity of the positive electrode does not increase more than a factor of 5 over the state of charge.
25. The lithium secondary cell of claim 1 or 2, wherein an electroactive material of the positive electrode comprises a lithium transition metal phosphate.
26. The lithium secondary cell of claim 25, wherein the transition metal of the lithium transition metal phosphate comprises one or more of vanadium, chromium, manganese, iron, cobalt and nickel.
27. The lithium secondary cell of claim 25, wherein the lithium transition metal phosphate is of the formula (Li1-xZx)MPO4, where M is one or more of vanadium, chromium, manganese, iron, cobalt and nickel, and Z is one or more of titanium, zirconium, niobium, aluminum, or magnesium, and x ranges from about 0.005 to about 0.05.
28. The lithium secondary cell of claim 27, wherein Z is selected from the group consisting of zirconium and niobium.
29. The lithium secondary cell of claim 1 or 2, wherein the positive electrode has a specific surface area of greater than about 10 m2g.
30. The lithium secondary cell of claim 1 or 2, wherein the positive electrode has a specific surface area of greater than about 15 m2g.
31. The lithium secondary cell of claim 1 or 2, wherein the positive electrode has a specific surface area of greater than about 20 m2g.
32. The lithium secondary cell of claim 1 or 2, wherein the positive electrode has a specific surface area of greater than about 30 m2g.
33. The lithium secondary cell of claim 1 or 2, wherein the position electrode has pore volume in the range of about 40% to about 70% by volume.
34. The lithium secondary cell of claim 1 or 2, wherein the positive electrode has thickness in the range of about 50 \u03bcm to about 125 \u03bcm.
35. The lithium secondary cell of claim 1 or 2, wherein the negative electrode comprises carbon.
36. The lithium secondary cell of claim 35, wherein the negative electrode comprises graphitic carbon.
37. The lithium secondary cell of claim 35, wherein the carbon is selected from the group consisting of graphite, spheroidal graphite, mesocarbon microbeads and carbon fibers.
38. The lithium secondary cell of claim 35, wherein the carbon has an average particle size of less than about 25 \u03bcm.
39. The lithium secondary cell of claim 35, wherein the carbon has an average particle size of less than about 15 \u03bcm.
40. The lithium secondary cell of claim 35, wherein the carbon has an average particle size of less than about 10 \u03bcm.
41. The lithium secondary cell of claim 35, wherein the carbon has an average particle size of less than about 6 \u03bcm.
42. The lithium secondary cell of claim 35, wherein the negative electrode has pore volume in the range of about 20 and 40% by volume.
43. The lithium secondary cell of claim 35, wherein the negative electrode has thickness in the range of about 20 \u03bcm to about 75 \u03bcm.
44. The lithium secondary cell of claim 35, wherein the carbon has a fast diffusion direction parallel to the long dimension of the particle with a dimension less than 6*(diffusion coefficient of fast directiondiffusion coefficient of MCMB)0.5 and a thickness less than about 75 microns and a porosity greater than 25%.
45. A method of charging a lithium secondary cell, comprising:
(a) providing a lithium secondary cell, comprising:
a high capacity lithium-containing positive electrode in electronic contact with a positive electrode current collector, said current collector in electrical connection with an external circuit;
a high capacity negative electrode in electronic contact with a negative electrode current collector, said current collector in electrical connection with an external circuit;
a separator positioned between and in ionic contact with the cathode and the anode; and
an electrolyte in ionic contact with the positive and negative electrodes,
wherein the total area specific impedance for the cell and the relative area specific impedances for the positive and negative electrodes are such that, during charging at greater than or equal to 4C, the negative electrode potential is above the potential of metallic lithium; and
(b) charging the cell at a C-rate of at least 4C, wherein at least 95% state of charge is obtained in less than 15 minutes.
46. The method of claim 45, comprising charging the cell at a C-rate of 10C, wherein at least 90% state of charge is obtained in less than 6 minutes.
47. The method of claim 45, comprising charging the cell at a C-rate of 20C, wherein at least 80% state of charge is obtained in less than 3 minutes.
48. The method of claim 45, wherein the cell is charged at an overpotential.
49. The method of claim 45, wherein the cell is charged at a potential near the oxidation potential of the electrolyte.
50. A low fade lithium secondary cell, comprising:
a lithium-containing positive electrode, said positive electrode in electronic contact with a positive electrode current collector, said current collector in electrical connection with an external circuit;
a negative electrode in electronic contact with a negative electrode current collector, said current collector in electrical connection with an external circuit;
a separator positioned between and in ionic contact with the cathode and the anode; and
an electrolyte in ionic contact with the positive and negative electrodes,
wherein the total area specific impedance for the cell and the relative area specific impedances for the positive and negative electrodes are such that the cell is capable of achieving at least about 80% state of charge within about 25 minutes, and
wherein the cell is capable of multiple chargedischarge cycles with a capacity loss of less than about 0.2% per cycle.
51. The cell of claim 50, wherein the cell is capable of achieving at least about 90% state of charge within about 12 minutes, and wherein the cell is capable of multiple chargedischarge cycles with a capacity loss of less than about 0.1% per cycle.
52. The cell of claim 50, wherein the cell is capable of achieving at least about 95% state of charge within about 6 minutes, and wherein the cell is capable of multiple chargedischarge cycles with a capacity loss of less than about 0.05% per cycle.

1461092304-d269f2a5-2be8-4020-ad20-4e90b0910ce6

The invention claimed is:

1. A nonwoven fabric comprising fibers of a resin composition comprising a cationic resin and an anionic resin.
2. The nonwoven fabric as claimed in claim 1, wherein the fibers are those formed from a resin composition comprising a regenerated cellulose, a cationic resin and an anionic resin.
3. The nonwoven fabric as claimed in claim 2, wherein, in said resin composition, the regenerated cellulose is contained in an amount of 20 to 98% by weight, the cationic resin is contained in an amount of 1 to 79% by weight, and the anionic resin is contained in an amount of 1 to 79% by weight.
4. The nonwoven fabric as claimed in claim 2, wherein said regenerated cellulose is at least one resin selected from the group consisting of viscose rayon, polynosic rayon, cupra and saponified acetate.
5. The nonwoven fabric as claimed in claim 2, wherein said cationic resin is at least one resin selected from the group consisting of cationized cellulose, cationized starch, cationized cyamposis gum, cationized dextrin and poly(dimethylmethylenepiperidinium chloride).
6. The nonwoven fabric as claimed in claim 1, comprising:
fibers of the resin composition comprising a regenerated cellulose, the cationic resin and the anionic resin, and
water-indecomposable short fibers.
7. The nonwoven fabric as claimed in claim 6, wherein, in said resin composition, the regenerated cellulose is contained in an amount of 20 to 98% by weight, the cationic resin is contained in an amount of 1 to 79% by weight, and the anionic resin is contained in an amount of 1 to 79% by weight.
8. The nonwoven fabric as claimed in claim 6, wherein said water-indecomposable short fibers are regenerated cellulose fibers having an average fiber length of less than 80 mm.
9. The nonwoven fabric as claimed in claim 6, wherein said regenerated cellulose is at least one resin selected from the group consisting of viscose rayon, polynosic rayon, cupra and saponified acetate.
10. The nonwoven fabric as claimed in claim 9, wherein said anionic resin is at least one resin selected from the group consisting of polyacrylic acid salt, carboxymethyl cellulose, carboxymethyl starch, alginic acid, xanthane gum and polymethacrylic acid salt.
11. The nonwoven fabric as claimed in claim 6, wherein said cationic resin is at least one resin selected from the group consisting of cationized cellulose, cationized starch, cationized cyamoposis gum, cationized dextrin and poly(dimethylmethylenepiperidinium chloride).
12. The nonwoven fabric as claimed in claim 6, wherein said anionic resin is at least one resin selected from the group consisting of polyacrylic acid salt, carboxymethyl cellulose, carboxymethyl starch, alginic acid, xanthane gum and polymethacrylic acid salt.
13. The nonwoven fabric as claimed in claim 1, wherein said cationic resin is at least one resin selected from the group consisting of cationized cellulose, cationized starch, cationized cyamoposis gum, cationized dextrin and poly(dimethylmethylenepiperidinium chloride).
14. The nonwoven fabric as claimed in claim 1, wherein said anionic resin is at least one resin selected from the group consisting of polyacrylic acid salt, carboxymethyl cellulose, carboxymethyl starch, alginic acid, xanthane gum and polymethacrylic acid salt.
15. The nonwoven fabric as claimed in claim 1, which has water decomposability.
16. A body fluid absorber having an absorbing layer comprising at least one nonwoven fabric selected from the group consisting of:
(a) a nonwoven fabric comprising fibers formed from a resin composition comprising a cationic resin and an anionic resin,
(b) a nonwoven fabric comprising fibers formed from a resin composition comprising a regenerated cellulose, a cationic resin and an anionic resin, and
(c) a nonwoven fabric comprising fibers formed from a resin composition comprising a regenerated cellulose, a cationic resin and an anionic resin, and water-indecomposable short fibers.
17. A wet tissue comprising:
at least one nonwoven fabric selected from the group consisting of:
(a) a nonwoven fabric comprising fibers formed from a resin composition comprising a cationic resin and an anionic resin,
(b) a nonwoven fabric comprising fibers formed from a resin composition comprising a regenerated cellulose, a cationic resin and an anionic resin, and
(c) a nonwoven fabric comprising fibers formed from a resin composition comprising a regenerated cellulose, a cationic resin and an anionic resin, and water-indecomposable short fibers; and

a liquid agent with which said nonwoven fabric is impregnated.

The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.

1. A method of coating multiple layers on a support comprising
a) taking a support;
b) simultaneously coating on said support a first chill settable layer and a non-chill settable layer, wherein the first chill settable layer is layered on top of the non-chill settable layer;
c) lowering the temperature of the layers to immobilize said layers; and
d) drying said layers, wherein the resulting product is an imaging element.
2. The method of claim 1 wherein the temperature is lowered to less than 30\xb0 C.
3. The method of claim 1 wherein the temperature is lowered to less than 20\xb0 C.
4. The method of claim 1 wherein the temperature is lowered to less than 10\xb0 C.
5. The method of claim 1 wherein a second chill settable layer is coated below the non-chill settable layer.
6. The method of claim 5 wherein the second chill settable layer is coated simultaneously with the non-chill settable layer and the first chill settable layer.
7. The method of claim 1 wherein the first chill settable layer comprises gelatin.
8. The method of claim 5 wherein the second chill settable layer comprises gelatin.
9. The method of claim 1 wherein the chill settable layer has a wet laydown thickness greater than 20% of the wet laydown thickness of the non-chill settable layer.
10. The method of claim 1 wherein the first chill settable layer and the non-chill settable layer are simultaneously coated with a multi-slotted slide hopper.
11. The method of claim 1 wherein the support absorbs water or wherein there is an additional layer coated on the support that absorbs water.
12. The method of claim 11 wherein there is an additional water absorbing layer coated on the support, said layer comprising gelatin.
13. The method of claim 1 wherein the non-chill settable layer is porous after drying.
14. The method of claim 1 wherein the first chill settable layer comprises sub-layers.
15. The method of claim 14 wherein chill settable sub-layers have different compositions.
16. The method of claim 15 wherein the chill settable sub-layers form an inner chill settable sub-layer and an outer chill settable sub-layer and wherein the outer chill settable sub-layer has a modulus greater than the modulus of the inner chill settable sub-layer after being coated and dried.
17. The method of claim 16 wherein the inner chill settable sub-layer has a modulus of less than 3 Gpa.
18. The imaging element of claim 16 wherein the outer chill settable sub-layer has a modulus of greater than 3 Gpa.
19. The method of claim 1 wherein the layers are dried at a temperature of less than 50\xb0 C.
20. A method of coating multiple layers on a support comprising
a) taking a support;
b) simultaneously coating on said support a first chill settable layer and a non-chill settable layer;
c) lowering the temperature of the layers to immobilize said layers; and
d) drying said layers, wherein the resulting product is an imaging element and the non-chill settable layer forms an image forming unit comprising photosensitive microcapsules and a developer.
21. The method of claim 20 wherein the imaging element is pressure developable.