1460773609-a83597bd-0098-40d7-9386-d9e2079e68dd

1. A process for producing a high melt flow index polymer, said high melt flow index polymer having a melt flow index of at least 300 dgmin and containing less than 300 ppm of a residual prodegradant, said process comprising the steps of:
providing a low melt flow index polymer;
adding at least one additive to said low melt flow index polymer;
adding at least one prodegradant to said low melt flow index polymer;
extruding said low melt flow index polymer in an extruder at an elevated temperature to initiate controlled molecular weight reduction of said low melt index polymer to form a high melt flow index polymer; and
quenching and pelletizing said high melt flow index polymer.
2. The process of claim 1, wherein said at least one prodegradant is dry mixed with said low melt flow index polymer prior to said extruding.
3. The process of claim 1, wherein said at least one prodegradant is added to said low melt flow index polymer as a solution during said extruding.
4. The process of claim 3, wherein said at least one prodegradant is added by injecting at the feed throat of an extruder.
5. The process of claim 3, wherein said at least one prodegradant is added by injecting into the barrel of an extruder.
6. The process of claim 1, wherein said high melt flow index polymer contains less than 50 ppm of a residual prodegradant.
7. The process of claim 1, wherein said at least one prodegradant comprises an organic peroxide.
8. The process of claim 1, wherein said at least one additive is selected from the group consisting of: anti-oxidants, processing stabilizers, and acid scavengers.
9. The process of claim 1, further comprising the step of removing unreacted prodegradant from said high melt flow index polymer.
10. The process of claim 9, wherein said unreacted prodegradant is removed by vacuum devolitazation.
11. The process of claim 10, wherein said vacuum devolitazation is accomplished by applying a vacuum to the barrel of said extruder during extruding.
12. The process of claim 1, wherein said low melt flow index polymer has a melt flow index of 100 dgmin or less.
13. The process according to claim 1, wherein the residence time of the polymer in said extruder is less than 60 seconds.
14. The process of claim 1, wherein said extruding is performed at a temperature from about 325\xb0 F. to about 475\xb0 F.
15. The process of claim 1, wherein said prodegradant is added in a quantity of from about 0.2 to about 2.0 percent by weight, based on the weight of low melt index polymer.
16. The process of claim 1, wherein said low melt flow index polymer is a polypropylene.
17. The process of claim 16, wherein said polypropylene is a random or block copolymer.
18. The process of claim 16, wherein said polypropylene has a high isotacticity.
19. The process of claim 1, wherein said high melt flow index polymer has a molecular weight distribution of from about 1.9 to about 2.9.
20. A pelletized high melt flow index polymer having a melt flow index of at least 300 dgmin and containing a residual amount of prodegradant that is less than 300 ppm;
said high melt flow index polymer being produced by controlled degradation of a low melt flow index polymer;
said controlled degradation being accomplished by extruding a low melt flow index polymer with at least one prodegradant.
21. The pelletized high melt flow index polymer according to claim 20, having a melt flow index of from 300 dgmin to 1000 dgmin.
22. The pelletized high melt flow index polymer according to claim 20, containing less than 50 ppm of residual prodegradant.
23. The pelletized high melt flow index polymer according to claim 20, having a molecular weight distribution of less than 3.0.
24. The pelletized high melt flow index polymer according to claim 20, wherein said polymer is a polypropylene.
25. The pelletized high melt flow index polymer according to claim 24, wherein said polypropylene is an ethylenepropylene copolymer.
26. The pelletized high melt flow index polymer according to claim 24, wherein said polypropylene has a high isotacticity.

The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.

1. An optical-microwave-quantum transducer comprising:
a tapered optical fiber configured to transmit and receive optical signals; and
a cantilever comprising:
an optical cavity that includes a nanophotonic crystal, the optical cavity being configured to provide mechanical excitation in response to electromagnetic excitation induced by photons emitted from the tapered optical fiber; and
a mechanical coupler being configured to induce electrical modulation onto a superconducting cavity in response to the mechanical excitation and to provide mechanical excitation in response to electromagnetic excitation induced by photons from the superconducting cavity, wherein the optical cavity is further configured to provide electromagnetic excitation that induces optical modulation on the tapered optical fiber in response to the mechanical excitation.
2. The optical-microwave-quantum transducer of claim 1, wherein the optical cavity comprises a pair of nanophotonic crystals arranged in parallel and separated by a gap, wherein each of the pair of nanophotonic crystals has a row of holes.
3. The optical-microwave-quantum transducer of claim 2, further comprising a buffer coupled between a given one of the pair of nanophotonic crystals and the mechanical coupler.
4. The optical-microwave-quantum transducer of claim 3, wherein the mechanical coupler comprises a capacitor with a first plate coupled to the buffer and a second plate coupled to the superconducting cavity.
5. The optical-microwave-quantum transducer of claim 4, wherein the optical cavity is configured to vibrate in response to trapping the photons emitted from the tapered optical fiber.
6. The optical-microwave-quantum transducer of claim 5, wherein the first plate of the capacitor vibrates in response to vibrations of the optical cavity, and wherein vibration of the first plate of the capacitor induces the electrical modulation on the second plate of the capacitor.
7. The optical-microwave-quantum transducer of claim 2, wherein the mechanical coupler comprises a piezoelectric actuator coupled to the pair of nanophotonic crystals and to the superconducting cavity.
8. The optical-microwave-quantum transducer of claim 7, wherein the optical cavity is configured to apply a pressure to the piezoelectric actuator in response to trapping the photons emitted from the tapered optical fiber.
9. The optical-microwave-quantum transducer of claim 8, wherein the piezoelectric actuator is configured to induce a voltage onto the superconducting cavity in response to the pressure applied to the piezoelectric actuator.
10. The optical-microwave-quantum transducer of claim 1, wherein optical cavity comprises a two-dimensional photonic lattice that comprises at least 10 rows of holes, and the nanophotonic crystal comprises a plate, and the plate is coupled to a substrate of the mechanical coupler.
11. The optical-microwave-quantum transducer of claim 10, wherein the mechanical coupler comprises a vacuum gap capacitor comprising:
a first plate circumscribed by the substrate; and
a second plate separated from the first plate by a vacuum gap, the second plate being electrically coupled to the superconducting cavity.
12. The optical-microwave-quantum transducer of claim 11, wherein the mechanical coupler further comprises a set of anchors tethered to the substrate, wherein the set of anchors are configured to allow a twisting of the photonic lattice and the first plate of the vacuum gap capacitor about an axis of rotation.
13. The optical-microwave-quantum transducer of claim 12, wherein photons trapped in the photonic lattice cause the photonic lattice to shift in a first direction, thereby causing the first plate of the vacuum gap capacitor to shift in a second direction, opposite the first direction about the axis of rotation.
14. The optical-microwave-quantum transducer of claim 13, wherein shifting of the first plate of the vacuum gap capacitor causes the second plate of the vacuum gap capacitor to induce the electrical modulation onto the superconducting cavity.
15. The optical-microwave-quantum transducer of claim 11, wherein the mechanical coupler further comprises a set of rails tethered along opposing edges of the substrate, wherein the set of rails are configured to allow shifting of a center region of the photonic lattice and the first plate of the capacitor.
16. The optical-microwave-quantum transducer of claim 15, wherein photons trapped in the photonic lattice cause the photonic lattice to shift in a given direction, thereby causing the first plate of the vacuum gap capacitor to shift in the given direction.
17. An optical-microwave-quantum transducer comprising:
a cantilever comprising
a mechanical coupler that is electrically coupled to a superconducting cavity, the mechanical coupler being configured to mechanically excite in response to an electrical pulse induced by photons emitted from the superconducting cavity on the mechanical coupler; and
an optical cavity having at least two rows of holes formed in a nanophotonic crystal and being mechanically coupled to the mechanical coupler, wherein a given hole in the nanophotonic crystal has an axis that extends through a center of the given hole and intersects with a tapered optical fiber, wherein the optical cavity is configured to induce optical modulation on the tapered optical fiber in response to the mechanical excitation of the mechanical coupler.
18. The optical-microwave-quantum transducer of claim 17, wherein the optical cavity comprises a pair of nanophotonic crystals arranged in parallel and separated by a gap, wherein each of the pair of nanophotonic crystals has a row of the at least two rows of holes.
19. The optical-microwave-quantum transducer of claim 18, wherein the optical cavity includes a photonic lattice and the at least two rows of holes comprises at least 10 rows of holes, and the nanophotonic crystal comprises a plate, and the plate is coupled to a substrate of the mechanical coupler, wherein the mechanical coupler comprises a vacuum gap capacitor comprising:
a first plate circumscribed by the substrate; and
a second plate separated from the first plate by a vacuum gap, the second plate being electrically coupled to a resonance circuit of the superconducting circuit.
20. A system comprising:
a refrigeration unit that stores an optical-microwave-quantum transducer at superconducting temperatures, the optical-microwave-quantum transducer comprising:
a node configured to transmit and receive optical pulses on an optical channel comprising an optical fiber, wherein the node is external to the refrigeration unit: and
a cantilever comprising:
an optical cavity that includes a nanophotonic crystal, the optical cavity being configured to provide mechanical excitation in response to electromagnetic excitation induced by photons emitted from the optical fiber; and
a mechanical coupler being configured to induce electrical modulation onto a superconducting cavity in response to the mechanical excitation and to provide mechanical excitation in response to electromagnetic excitation induced by photons from the superconducting cavity, wherein the optical cavity is further configured to provide electromagnetic excitation that induces optical modulation on the optical fiber in response to the mechanical excitation.
21. The system of claim 20, wherein the node comprises another refrigeration unit that stores another optical-quantum transducer at superconducting temperatures.