1460774821-feabad73-68d5-4002-b493-38ab418054a9

1. A method of improving the properties of a metallic component for use in a corrosive environment comprising the steps of:
identifying at least one portion of the component that is expected to be exposed to a corrosive environment;
determining a desired compressive stress distribution for said at least one portion of the component that is expected to be exposed to a corrosive environment;
inducing said desired compressive stress distribution within at least a portion of the surface of a component.
2. The method of claim 1 wherein said desired compressive stress distribution having a magnitude, depth, and cold work effective to mitigate SCC and H2S cracking of the component during use in a corrosive environment.
3. The method of claim 1 wherein the corrosive environment is identified and wherein the desired compressive stress distribution is determined for the identified corrosive environment.
4. The method of claim 1, wherein said compressive stress distribution is induced using a CNC or robotically controlled burnishing and effective to impart the desired compressive stresses in a controlled manner.
5. The method of claim 1 wherein the step of inducing the desired compressive stress distribution includes using a hydraulically supported burnishing apparatus.
6. The method of claim 1 wherein the step of inducing the desired compressive stress distribution includes the steps of determining burnishing parameters to provide a smooth surface along the at least one portion of the surface of the component such that surface irregularities that can become crack or corrosion pit initiation sites are placed in compression
7. The method of claim 6 wherein said burnishing parameters include the smoothness of the burnishing member that will be used for inducing compressive stress within the at least one portion of the surface of the component, the diameter of the of the burnishing member, the force with which the burnishing member will be pressed against the at least one portion of the surface of the component, and the pattern of burnishing.
8. The method of claim 1 further comprises the step of identifying the material properties of the component, the applied loads expected to be applied to the component, the environment in which the component is expected to operate, and the known causes Of failure for similar components.
9. The method of claim 1 further comprising the step of enhancing the smoothness of the surface along the at least a portion of the surface of a component such that surface irregularities that can become crack or corrosion pit initiation sites are reduced or eliminated.
10. The method of claim 1 wherein the desired compressive stress has a magnitude and depth of compression that extends to a depth of at least nominally of about 0.5 mm such that the sum of residual and applied stress never exceeds the threshold for SCC in the corrosive environment of the application or the fatigue endurance limit of the material.
11. The method of claim 1 wherein the induced desired compressive stress has a depth of compression that incorporates a majority of surface irregularities along the at least one portion of the surface of the component.
12. The method of claim 1 wherein the desired compressive stress distribution has a depth of penetration that penetrates entirely through the at least a portion of the surface of a component.
13. The method of claim 1 wherein the compressive stress distribution within at least a portion of the surface of the component has a depth that exceeds the depth of any surface irregularities.
14. A component for use in a corrosive environment comprising:
at least one portion of the component having a metallic surface;
a compressive stress distribution within said surface;
wherein the depth of said compressive stress distribution is such that it exceeds a majority of surface irregularities along said surface and having an amount of cold work induced within said surface that is less than the amount necessary to damage the crystalline structure along said surface and to create slip bands, dislocations, and twinning such that said surface is more susceptible to stress corrosion.
15. The metallic component of claim 14 wherein the said surface has a depth of compression is at least about 1 mm.
16. The metallic component of claim 12 wherein said stress distribution has a magnitude and depth of compression at least as great as the sum of any residual and applied stress anticipated within said at least one portion.
17. The metallic component of claim 12 wherein said stress distribution has a depth of compression that does not exceed the threshold for SCC in the expected corrosive environment of the application of the component.
18. The metallic component of claim 12 wherein said at least one portion has a depth and said compressive stress distribution penetrates through the entire depth of the at least one portion.

The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.

1. A liquid crystal display panel comprising:
an upper substrate having a plurality of row lines formed thereon;
a lower substrate having a plurality of column lines formed thereon perpendicular to the plurality of column lines; and
a plurality of pixel regions formed at each crossed region of the plurality of column lines and the plurality of row lines; and column spacers each formed between the upper substrate and the lower substrate for maintaining a cell gap between the upper substrate and the lower substrate,
wherein the column spacers formed at a first region of a display region adjacent to a liquid crystal injection have dot shapes and the column spacers formed at a second region which is rest of the display region excluding the first region have dam shapes.
2. The liquid crystal display panel as claimed in claim 1, wherein, the column spacers in the shape of dam have the same length as the length of the pixel regions.
3. The liquid crystal display panel as claimed in claim 1, wherein, the column spacers in the shape of dot have a length shorter than a length of the pixel region.
4. The liquid crystal display panel as claimed in claim 1, wherein, a distance between adjacent column spacers is the same as a length of the pixel region.
5. The liquid crystal display panel as claimed in claim 4, wherein, a distance from the liquid crystal injection to the first region of the display region is in a range of 1 mm\u02dc7 mm.
6. The liquid crystal display panel as claimed in claim 5, wherein, the distance is in a range of 3 mm\u02dc5 mm.
7. The liquid crystal display panel as claimed in claim 4, wherein, a number of the column spacers in the first region are formed to be gradually more as it goes to a second region which is rest of the display region excluding the first region.
8. The liquid crystal display panel as claimed in claim 4, wherein, the width of the column spacers in the first region is formed to be gradually wider as it goes to a second region which is rest of the display region excluding the first region.
9. The liquid crystal display panel as claimed in claim 1, wherein, a distance between adjacent column spacers in the shape of dam is longer than a length of one pixel region, such that the column spacers in the shape of dam are formed in zigzag.
10. The liquid crystal display panel as claimed in claim 9, wherein, the column spacers in the shape of dam is formed alternately on the right side or left side of the pixel regions.
11. The liquid crystal display panel as claimed in claim 9, wherein, the column spacers in the shape of dam is formed alternately on the upper side or lower side of the pixel regions.
12. The liquid crystal display panel as claimed in claim 1, wherein, a distance between adjacent column spacers in the shape of dam is shorter than a length of one pixel region.
13. The liquid crystal display panel as claimed in claim 1, wherein a seal line for bonding the upper substrate and the lower substrate to define the display region.
14. The liquid crystal display panel as clamed in claim 1, wherein the column spacers in the shape of dam are arranged in parallel to a rubbing direction of an alignment layer