1460879796-68ab83e8-3904-4e6e-8432-8a7859fbbb03

1. A fuel cell roll good subassembly, comprising:
a plurality of individual electrolyte membranes, each electrolyte membrane comprising a center region;
one or more first subgaskets attached to the individual electrolyte membranes, each of the first subgaskets having at least one aperture, the first subgaskets arranged so that the center regions of the individual electrolyte membranes are exposed through the apertures of the first subgaskets;
a second subgasket comprising a web having a plurality of apertures, the second subgasket web arranged so that center regions of the individual electrolyte membranes are exposed through the apertures of the second subgasket web;
a first catalyst coated gas diffusion layer, wherein the one of the first subgaskets is positioned between the first catalyst coated gas diffusion layer and one of the electrolyte membranes; and
a second catalyst coated gas diffusion layer, wherein the one of the second subgasket is positioned between the second catalyst coated gas diffusion layer and one of the electrolyte membranes,
each of the one or more first subgaskets comprises a first subgasket layer having a first subgasket surface oriented toward the electrolyte membrane, the first subgasket having a first adhesive layer disposed on the first subgasket surface; and
the second subgasket comprises a second subgasket layer having a second subgasket surface oriented toward the electrolyte membrane, wherein a second adhesive layer is not disposed on substantial portions of the second subgasket surface
wherein the first gasket aperture and the second gasket aperture are different sizes.
2. The roll good subassembly of claim 1, wherein the first adhesive layer of each of the one or more first subgaskets is attached to the second subgasket surface.
3. The roll good subassembly of claim 1, wherein the one or more first subgaskets is one first subgasket comprising a web having a plurality of apertures.
4. The roll good subassembly of claim 1, wherein the first gasket aperture and the second gasket aperture are different sizes.
5. The fuel cell roll good subassembly of claim 4, wherein the first gasket aperture is smaller than the second gasket aperture.
6. A fuel cell roll good subassembly, comprising:
a plurality of individual electrolyte membranes, each electrolyte membrane comprising a center region, wherein at least some of the electrolyte membranes are catalyst coated electrolyte membranes comprising a first catalyst, a second catalyst, and an electrolyte membrane having first and second generally opposed major surfaces and first and second generally opposed edges, and wherein the first catalyst is on the first major surface, wherein the second catalyst is on the second major surface wherein the first and second generally opposed edges of at least one of the electrolyte membranes, first catalyst, and second catalyst are co-terminus;
one or more first subgaskets attached to the individual electrolyte membranes, each of the first subgaskets having at least one aperture, the first subgaskets arranged so that the center regions of the individual electrolyte membranes are exposed through the apertures of the first subgaskets; and
a second subgasket comprising a web having a plurality of apertures, the second subgasket web arranged so that center regions of the individual electrolyte membranes are exposed through the apertures of the second subgasket web,
wherein the catalyst coated electrolyte membrane is thrifted on at least 2 opposing sides and wherein each of the one or more first subgaskets comprises a first subgasket layer having a first subgasket surface oriented toward the individual electrolyte membranes, each of the one or more the first subgaskets having a first adhesive layer disposed on the first subgasket surface; and
the second subgasket comprises a second subgasket layer having a second subgasket surface oriented toward the individual electrolyte membranes, wherein a second adhesive layer is not disposed on substantial portions of the second subgasket surface.
7. The roll good subassembly of claim 6, wherein the first adhesive layer of each of the one or more first subgaskets is attached to the second subgasket surface.
8. The roll good subassembly of claim 6, wherein the one or more first subgaskets is one first subgasket comprising a web having a plurality of apertures.
9. The roll good assembly of claim 6, further comprising gas diffusion layers disposed over the center regions of the individual electrolyte membranes.
10. The fuel cell roll good subassembly of claim 6, wherein the first gasket aperture is smaller than the second gasket aperture.

The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.

1. A thiophene monomer having the following general formula:
9
wherein:
a) m is an integer ranging from 2 to 3;
b) R* is a quaternary ammonium;
c) Y is an oxygen atom or a methylene; and
d) R1 is a methyl group or a hydrogen atom.
2. A monomer as defined in claim 1, wherein:
a) m3;
b) R* is NEt3;
c) Y is an oxygen atom; and
d) R1 is a methyl group.
3. A monomer as defined in claim 1, wherein:
a) m is 2;
b) R* is
10
c) Y is an oxygen atom; and
d) R1 is a methyl group.
4. A monomer as defined in claim 1, wherein:
a) m is 2;
b) R* is
11
c) Y is an oxygen atom; and
d) R1 is a methyl group.
5. A monomer as defined in claim 1, wherein:
a) m is 2;
b) R* is
12
c) Y is a methylene group; and
d) R1 is a hydrogen atom.
6. The monomer as defined in claim 2, having the formula:
13
7. The monomer as defined in claim 3, having the formula:
14
8. The monomer as defined in claim 4, having the formula:
15
9. The monomer as defined in claim 5, having the formula:
16
10. A polymer comprising a plurality of monomeric units as defined in any one of claims 1 to 9.
11. A process for the preparation of a monomer as defined in claim 2, comprising:
a) reacting a molecule of formula 1:
17
with a reagent of formula 2:
18
in the presence of a copper halide, said reaction resulting in the formation of a first reaction mixture comprising a compound of formula 3:
19
b) isolating said compound of formula 3 from said first reaction mixture;
c) reacting said compound of formula 3 with ethylbromide, resulting in the formation of a second reaction mixture comprising said monomer; and
d) recovering said monomer from said second reaction mixture.
12. The process of claim 11, wherein said copper halide is Cul.
13. A process for the preparation of a monomer as defined in claim 3, comprising:
a) reacting a compound of formula 4:
20
with 1-methylimidazole, resulting in the formation of a reaction mixture; and
b) recovering said monomer from said reaction mixture.
14. A process for the preparation of a monomer as defined in claim 4, comprising:
a) reacting a compound of formula 4:
21
with 1,2-dimethylimidazole, resulting in the formation of a reaction mixture; and
b) recovering said monomer from said reaction mixture.
15. A process for the preparation of a monomer as defined in claim 5, comprising:
a) reacting a compound of formula 6:
22
with 1-methylimidazole, resulting in the formation of a reaction mixture; and
b) recovering said monomer from said reaction mixture.
16. A process for polymerizing the monomer defined in any one of claims 1 to 9, comprising reacting said monomer in the presence of an oxidizing agent, resulting in the formation of a polymer of the following general formula:
23
wherein:
a) m is an integer ranging for 2 to 3;
b) n is an integer ranging from 3 to 100;
c) R* is a quaternary ammonium;
d) Y is an oxygen atom or a methylene; and
e) R1 is a methyl group or a hydrogen atom.
17. The process of claim 16, wherein said oxidizing agent is FeCl3 or K2S2O8.
18. The process of claim 16, wherein when R1 is a methyl group, said polymer is regio-regular and water soluble.
19. The process of claim 18, wherein said polymer is thermostable.
20. A polymer obtained from the process of anyone of claims 16 to 18.
21. A method for detecting the presence of a negatively charged polymer, comprising the steps of:
a) contacting a complementary target to said polymer with a polymer as defined in claim 20 to form a duplex;
b) contacting said duplex with said negatively charged polymer; and
c) detecting a change in electronic charge, fluorescence or color as an indication of the presence of said negatively charged polymer.
22. A method as defined in claim 21, wherein said negatively charged polymer is selected from the group consisting of: acidic proteins, glycosaminoglycans, hyaluronans, heparin, chromatographic substrates, culture substrates and nucleic acids.
23. A method as defined in claim 22, wherein said negatively charged polymer is a nucleic acid.
24. A method as defined in claim 23, wherein said nucleic acid is DNA.
25. A method as defined in claim 23, wherein said nucleic acid is RNA.
26. A method as defined in claim 23, wherein said complementary target is a nucleic acid complementary to said negatively charged polymer.
27. A method as defined in claim 26, wherein said complementary target is a nucleic acid probe and said negatively charged polymer is a denatured PCR amplicon.
28. A method for discriminating a first nucleic acid from a second nucleic acid, said second nucleic acid differing from said first nucleic acid by at least one nucleotide, comprising the steps of:
e) contacting a complementary target to said first nucleic acid with a polymer as defined in claim 20 to form a duplex;
f) contacting said duplex with said first nucleic acid, resulting in specific hybridization;
g) contacting said duplex with said second nucleic acid, resulting in non-specific hybridization; and
h) detecting a change in electronic charge, fluorescence or color.
29. A method as defined in claim 28, wherein said change in electronic charge, fluorescence or color is more pronounced with said specific hybridization.
30. A method as defined in claim 29, wherein said complementary target is a nucleic acid complementary to said first nucleic acid.
31. A method as defined in claim 30, wherein said first nucleic acid and said second nucleic acid are DNA.
32. A method as defined in claim 30, wherein said first nucleic acid and said second nucleic acid are RNA.
33. A method as defined in claim 30, wherein said complementary target is a nucleic acid probe and said first nucleic acid and said second nucleic acid are denatured PCR amplicons.
34. Use of a positively charged polymer comprising a repeating thiophene moiety for detecting the presence of a negatively charged polymer.
35. A use as defined in claim 34, wherein said positively charged polymer is reacted with a complementary target to said negatively charged polymer.
36. A use as defined in claim 35, wherein said positively charged polymer is ionically linked to said complementary target.
37. A use as defined in claim 34, wherein a complementary target to said negatively charged polymer is linked to a solid support, said negatively charged polymer is then reacted with said complementary target which results in its capture by said solid support resulting in the formation of a complex and then said positively charged polymer is reacted with said complex of said complementary target with said negatively charged polymer.
38. A use as defined in claim 34, wherein a complementary target to said negatively charged polymer is linked to a solid support, said positively charged polymer is then reacted with said complementary target resulting in its capture by said solid support forming a complex, and then reacting said negatively charged polymer with said complex of said complementary target and said positively charged polymer.
39. A use as defined in claim 37 or 38, wherein said solid support is selected from the group consisting of an electrode, an optical fiber, a glass slide and glass beads.
40. A use as defined in any one of claims 37-39 for purifying negatively charged polymers.
41. A use as defined in claim 40, wherein said negatively charged polymers are nucleic acids.