1. A coated overhead conductor comprising an assembly including one or more conductive wires, wherein the assembly comprises an outer surface coated with an electrochemical deposition coating forming an outer layer, wherein the electrochemical deposition coating comprises a first metal oxide, wherein the first metal oxide is not aluminum oxide.
2. The coated overhead conductor of claim 1, wherein the first metal oxide comprises titanium oxide, zirconium oxide, zinc oxide, niobium oxide, vanadium oxide, molybdenum oxide, copper oxide, nickel oxide, magnesium oxide, beryllium oxide, cerium oxide, boron oxide, gallium oxide, hafnium oxide, tin oxide, iron oxide, yttrium oxide or combinations thereof.
3. The coated overhead conductor of claim 1, wherein the one or more conductive wires are formed of aluminum or aluminum alloy.
4. The coated overhead conductor of claim 3, wherein the outer layer is further formed of a second metal oxide, wherein the second metal oxide is aluminum oxide.
5. The coated overhead conductor of claim 1, wherein the one or more conductive wires are formed of copper or copper alloy.
6. The coated overhead conductor of claim 2, wherein the first metal oxide comprises titanium oxide, zirconium oxide or combinations thereof.
7. The coated overhead conductor of claim 1 having a lower operating temperature compared to the operating temperature of an uncoated overhead conductor at similar operating conditions.
8. The coated overhead conductor of claim 1, wherein the electrochemical deposition coating is non-white.
9. The coated overhead conductor of claim 1, wherein the outer layer has a thickness of about 1 micron or more.
10. The coated overhead conductor of claim 1, wherein the outer layer has a thickness of about 5 microns to about 25 microns.
11. The coated overhead conductor of claim 1, wherein the outer layer has a thickness variation of about 3 microns or less.
12. The coated overhead conductor of claim 1 having an operating temperature reduced by at least 5\xb0 C. when compared to the operating temperature of an uncoated overhead conductor at similar operating conditions.
13. The coated overhead conductor of claim 1 having an operating temperature reduced by at least 10\xb0 C. when compared to the operating temperature of an uncoated overhead conductor, when the operating temperatures measured are above 100\xb0 C. and at similar operating conditions.
14. The coated overhead conductor of claim 1 having reduced power transmission loss when compared to an uncoated overhead conductor at similar operating conditions.
15. The coated overhead conductor of claim 1 having increased current carrying capacity when compared to an uncoated overhead conductor at similar operating conditions.
16. The coated overhead conductor of claim 3, wherein the one or more conductive wires are formed from an aluminum alloy selected from the group consisting of 1350 alloy aluminum, 6000-series alloy aluminum, aluminum-zirconium alloy, and combinations thereof.
17. The coated overhead conductor of claim 1, wherein at least some of the one or more conductive wires have trapezoidal cross-sections.
18. The coated overhead conductor of claim 1, wherein the one or more conductive wires surround a core comprised of steel, carbon fiber composite, glass fiber composite, carbon nanotube composite, or aluminum alloy.
19. The coated overhead conductor of claim 1, wherein each of the conductive wires is individually coated with the electrochemical deposition coating.
20. The coated overhead conductor of claim 1, wherein a portion of each of the conductive wires is coated with the electrochemical deposition coating.
21. The coated overhead conductor of claim 1, wherein the electrochemical deposition coating is electrically non-conductive.
22. A method for making a coated overhead conductor, the method comprising:
a. providing a bare conductor; and
b. performing electrochemical deposition of a first metal oxide on an outer surface of the bare conductor to form an outer layer on the bare conductor, the outer layer comprising an electrochemical deposition coating, wherein the first metal oxide is not aluminum oxide.
23. The method of claim 22, wherein the electrochemical deposition coating is non-white.
24. The method of claim 22, wherein the first metal oxide is titanium oxide, zirconium oxide, zinc oxide, niobium oxide, vanadium oxide, molybdenum oxide, copper oxide, brass oxide, nickel oxide, magnesium oxide, beryllium oxide, cerium oxide, boron oxide, gallium oxide, hafnium oxide, tin oxide, iron oxide, yttrium oxide, or combinations thereof.
25. The method of claim 22, wherein the outer layer has a thickness of about 1 micron to about 25 microns.
26. The method of claim 22, wherein the outer layer has a thickness variation of about 3 microns or less.
27. The method of claim 22, wherein the coated overhead conductor has an operating temperature reduced by at least 5\xb0 C. compared to the operating temperature of an uncoated overhead conductor at similar operating conditions.
28. The method of claim 22, wherein the coated overhead conductor has an operating temperature reduced by at least 10\xb0 C. compared to the operating temperature of an uncoated overhead conductor, when the operating temperatures is above 100\xb0 C. at similar operating conditions.
29. The method of claim 22, wherein the coated overhead conductor has reduced power transmission loss when compared to an uncoated overhead conductor at similar operating conditions.
30. The method of claim 22, wherein the coated overhead conductor has increased current carrying capacity when compared to an uncoated overhead conductor at similar operating conditions.
31. The method of claim 22, wherein the bare conductor comprises a plurality of conductor wires made from one or more of copper, copper alloy, aluminum, or aluminum alloy.
32. The method of claim 31, wherein the plurality of conductive wires are formed from an aluminum alloy comprising 1350 alloy aluminum, 6000-series alloy aluminum, or aluminum-zirconium alloy.
33. The method of claim 22, wherein the bare conductor comprises a plurality of conductive wires, wherein at least some of the plurality of conductive wires have a trapezoidal cross-section.
34. The method of claim 22, wherein the bare conductor comprises a plurality of conductive wires stranded around a core, and wherein the core is comprises steel, carbon fiber composite, glass fiber composite, carbon nanotube composite, or aluminum alloy.
35. The method of claim 22, wherein the bare conductor is formed of a plurality of conductive wires, and wherein the electrochemical deposition coats only an outer surface of the bare conductor.
36. The method of claim 22, wherein the bare conductor comprises a plurality of conductive wires, and wherein the electrochemical deposition coats each of the conductive wires.
37. The method of claim 22, wherein the electrochemical deposition coats only a portion of the bare conductor.
38. The method of claim 22, wherein the electrochemical deposition coating is electrically non-conductive.
39. The method of claim 22 being continuous, semi-continuous, or batch.
40. The method of claim 22, wherein the performance of the electrochemical deposition comprises:
i. providing an aqueous solution containing at least one of water-soluble complex metal fluorides, water-dispersible complex metal fluorides, water-soluble complex metal oxyfluorides, and water-dispersible metal oxyfluorides;
ii. providing a cathode in contact with said aqueous solution;
iii. placing the bare conductor in the aqueous solution as an anode;
iv. passing a current between the anode and the cathode through the aqueous solution to form the electrochemical deposition coating on the outer surface of the bare conductor; and
v. removing the coated overhead conductor from the aqueous solution.
41. The method of claim 40, wherein the current is pulsed.
42. The method of claim 40, wherein the current is from about 10 ampssquare foot to about 400 ampssquare foot.
43. The method of claim 40, wherein the metal is titanium or zirconium.
44. The method of claim 22, wherein the metal oxide is titanium oxide or zirconium oxide.
45. A coated overhead conductor comprising an assembly including one or more conductive wires, wherein the one or more conductive wires are formed of aluminum or aluminum alloy, wherein the assembly comprises an outer surface coated with an electrochemical deposition coating forming an outer layer, the electrochemical deposition coating comprises titanium oxide, zirconium oxide or combinations thereof, and the outer layer has a thickness from about 5 microns to about 25 microns.
The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.
1. In combination with a boat anchor having a protruding stock, an anchor protector for minimizing damage from impact with the protruding stock, comprising:
a conical impact absorber formed from a plastic material, the impact absorber comprising a base end and an apex end, the base end terminating in a substantially planar base;
a cylindrical neck formed from a plastic material integrally with the impact absorber, the neck extending outwardly from the apex end, terminating in a substantially planar cap opposite to the apex end;
a sleeve extending inwardly from the cap along the longitudinal axis of the impact absorber, the sleeve adapted for receiving the protruding stock and removably attaching the anchor protector to the protruding stock by way of a force of friction.
2. The anchor protector as in claim 1, wherein the plastic material is high impact polystyrene.
3. The anchor protector as in claim 2, wherein the anchor protector has positive buoyancy.
4. The anchor protector as in claim 3, wherein said positive buoyancy is achieved by an airtight cavity formed inside the impact absorber.