1460884632-321726c3-cc13-4c04-bc31-0a72d0ae81ae

1. A fixing member, comprising:
a fixing rotational body having a heat source built therein, wherein:
the fixing rotational body is configured to fix unfixed toner onto a recording medium as the recording medium carrying the unfixed toner passes through a nip portion formed between the fixing rotational body and a pressurizing unit that comes into pressure contact with the fixing rotational body via the recording medium,
the fixing member is made of silicon rubber having carbon fiber, wherein a plurality of vacant spaces are formed in the silicon rubber;
the carbon fiber is a pitch type carbon fiber,
the carbon fiber has a shape in which a length of the carbon fiber is longer than a diameter of the vacant spaces,
a part of the carbon fiber is provided inside the vacant spaces, and other part of the carbon fiber is provided inside a bubble continuation part connecting the vacant spaces to each other not adhered to the silicon rubber, and
the carbon fibers in the silicon rubber contact each other to form paths for transferring heat.
2. A fixing rotational body comprising the fixing member according to claim 1.
3. The fixing rotational body according to claim 2, comprising:
a cored bar which is a metal roller, wherein:
the cored bar has a thickness that is greater than or equal to 0.25 mm and less than or equal to 0.5 mm; and
plural projections having circling shapes are formed on an inner surface of the cored bar.
4. The fixing rotational body according to claim 2 comprising:
a layer made of fluorine polymer, which is provided on an outermost surface of the fixing rotational body.
5. The fixing rotational body according to claim 2 wherein:
the fixing rotational body has a surface roughness Rz (ten point average roughness) of less than or equal to 5 \u03bcm.
6. A fixing device comprising the fixing rotational body according to claim 2.
7. An image forming apparatus comprising:
the fixing device according to claim 6; and
an image forming unit, wherein:
a toner image is formed on a recording medium at the image forming unit; and
the toner image is fixed onto the recording medium at the fixing device.

The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.

1. A PE tarpaulin prepared by coating low-density polyethylene on both surfaces of a main material cloth woven to have partial overlap yarn structures by periodically overlapping in weft and warp directions two flat yarns prepared by mixing 30 to 50 wt % of high-density polyethylene and 70 to 50 wt % of polypropylene homo polymer in 100 wt % of flat yarns which are drawing yarns.
2. The PE tarpaulin of claim 1, wherein a melting index of high-density polyethylene measured at 190\xb0 C. with a load of 2.16 kg ranges from 0.6 to 1.2 g10 min.
3. The PE tarpaulin of claim 1, wherein a melting index of polypropylene homo polymer measured at 230\xb0 C. with a load of 2.16 kg ranges from 1.5 to 3.5 g10 min.
4. The PE tarpaulin of claim 1, wherein, when the cloth is woven by using the flat yarns, wefts and warps have partial overlap yarn structures, and a density of the overlap yarn structures is 3 to 6 per 1 inch of weft and warp.