1460885988-fb3f483f-a5e7-4ac8-9585-ad7c2ff64caf

1. A method of forming a layer over a substrate, comprising:
providing a supercritical fluid comprising a precursor dispersed therein;
providing a reaction chamber having a substrate therein, the substrate having a surface; and
flowing the supercritical fluid having precursor dispersed therein into the reaction chamber; the precursor interacting with the surface of the substrate to form a monolayer over at least a portion of the surface of the substrate.
2. The method of claim 1 wherein the precursor is part of a mixture of precursors dispersed within the supercritical fluid, and two or more precursors from the mixture interact with the surface of the substrate to form the monolayer.
3. The method of claim 2 wherein the precursors within the mixture of precursors comprise an aluminum-containing precursor and a hafnium-containing precursor.
4. The method of claim 2 wherein the precursors within the mixture of precursors consist essentially of an aluminum-containing precursor and a hafnium-containing precursor.
5. The method of claim 2 wherein the precursors within the mixture of precursors comprise a titanium-containing precursor and a tantalum-containing precursor.
6. The method of claim 2 wherein the precursors within the mixture of precursors consist essentially of a titanium-containing precursor and a tantalum-containing precursor.
7. The method of claim 6 wherein a ratio of the titanium-containing precursor to the tantalum-containing precursor is from about 5:95 to about 10:90.
8. The method of claim 6 wherein the titanium-containing precursor is TiF5 or titanium isopropoxide, and the tantalum-containing precursor is pentakis(dimethylamino)tantalum, TaF5 or tantalum ethoxide.
9. The method of claim 1 wherein the precursor comprises a metal.
10. The method of claim 1 wherein the precursor has a vapor pressure of less than or equal to about 0.1 Torr at 100\xb0 C.
11. The method of claim 1 wherein the precursor comprises a metal halide and wherein the supercritical fluid predominately comprises CO2.
12. The method of claim 1 wherein the precursor comprises hafnium, titanium or tantalum.
13. The method of claim 1 wherein the precursor is TiF5, titanium isopropoxide, pentakis(dimethylamino)tantalum, TaF5, tantalum ethoxide, or HfCl4.
14. The method of claim 1 wherein one or more conditions within the reaction chamber are below critical conditions of the supercritical fluid during formation of at least some of the monolayer so that the supercritical fluid is not in a supercritical state within the reaction chamber during formation of at least some of the monolayer.
15. The method of claim 14 wherein the one or more conditions within the reaction chamber which are below the critical conditions of the supercritical fluid include a pressure which is below the critical pressure of the supercritical fluid.
16. The method of claim 14 wherein the one or more conditions within the reaction chamber are below the critical conditions as the supercritical fluid is flowed into the chamber so that the supercritical fluid transforms to the non-supercritical state upon being flowed into the chamber.
17. The method of claim 14 wherein:
the supercritical fluid is flowed into the chamber in the supercritical state and under conditions suitable to maintain the supercritical fluid in the supercritical state; and
after the supercritical fluid is flowed into the reaction chamber, conditions within the reaction chamber are changed to reduce the one or more conditions within the reaction chamber to below the critical conditions of the supercritical fluid.
18. A method of depositing material over a substrate, comprising:
providing a first precursor and a second precursor different from the first precursor;
providing an atomic layer deposition reaction chamber having a substrate therein, the substrate having a surface;
performing at least one iteration of the following sequence:
flowing the first precursor into the chamber to form a first component deposited over a surface of the substrate;
after forming the first component, purging substantially all of any of the first precursor remaining free in the chamber from the chamber;
after purging substantially all of the first precursor from the reaction chamber, flowing the second precursor into the chamber to form a second component over the surface of the substrate;
after forming the second component, purging substantially all of any of the second precursor remaining free in the chamber from the chamber; and

wherein at least one of the first and second precursors is dispersed in a supercritical fluid as it is flowed into the reaction chamber.
19. The method of claim 18 wherein the first precursor is dispersed in the supercritical fluid as it is flowed into the reaction chamber.
20. The method of claim 19 wherein the first precursor comprises a metal.
21. The method of claim 19 wherein the first precursor has a vapor pressure of less than or equal to about 0.1 Torr at 100\xb0 C.
22. The method of claim 19 wherein the first precursor comprises a metal halide and wherein the supercritical fluid predominately comprises CO2.
23. The method of claim 19 wherein the first precursor comprises hafnium, aluminum, titanium or tantalum.
24. The method of claim 18 wherein the second precursor is dispersed in the supercritical fluid as it is flowed into the reaction chamber.
25. The method of claim 18 wherein the first and second precursors are both dispersed in supercritical fluids as they are flowed into the reaction chamber.
26. The method of claim 18 wherein:
the first precursor comprises a metal;
the first component comprises the metal;
the second precursor comprises nitrogen; and
the second component comprises the nitrogen.
27. The method of claim 18 wherein:
the first precursor comprises a metal;
the first component comprises the metal;
the second precursor comprises oxygen; and
the second component comprises the oxygen.
28. The method of claim 27 wherein:
the first precursor comprises hafnium;
the first component comprises hafnium from the first precursor; and
the oxygen of the second precursor reacts with the hafnium of the first component to form hafnium oxide.
29. The method of claim 28 wherein the first precursor is HfCl4 and the second precursor is H2O or O3.
30. The method of claim 27 wherein:
the first precursor is part of a mixture of precursors;
the precursors within the mixture comprise two or more different metals; and
the first component comprises the two or more different metals.
31. The method of claim 28 wherein the mixture of precursors consists essentially of an aluminum-containing precursor and a hafnium-containing precursor.
32. The method of claim 28 wherein the mixture of precursors consists essentially of a titanium-containing precursor and a tantalum-containing precursor.
33. The method of claim 32 wherein a ratio of the titanium-containing precursor to the tantalum-containing precursor is from about 5:95 to about 10:90, by atomic percent.
34. The method of claim 32 wherein the titanium-containing precursor is TiF5 or titanium isopropoxide, and the tantalum-containing precursor is TaF5, tantalum ethoxide or pentakis(dimethylamino)tantalum.
35. The method of claim 18 wherein one or more conditions within the reaction chamber are below critical conditions of the supercritical fluid during at least some of the time that the supercritical fluid is within the reaction chamber so that the supercritical fluid transforms to a non-supercritical state within the reaction chamber.
36. The method of claim 35 wherein the one or more conditions within the reaction chamber which are below the critical conditions of the supercritical fluid include a pressure which is below the critical pressure of the supercritical fluid.
37. The method of claim 35 wherein the one or more conditions within the reaction chamber are below the critical conditions as the supercritical fluid is flowed into the chamber so that the supercritical fluid transforms to the non-supercritical state upon being flowed into the chamber.
38. The method of claim 35 wherein:
the supercritical fluid is flowed into the chamber in the supercritical state and under conditions suitable to maintain the supercritical fluid in the supercritical state; and
after the supercritical fluid is flowed into the reaction chamber, conditions within the reaction chamber are changed to reduce the one or more conditions within the reaction chamber to below the critical conditions of the supercritical fluid.
39. A method of depositing material over a substrate, comprising:
providing a supercritical fluid comprising a first precursor dispersed therein;
providing a second precursor;
providing an atomic layer deposition reaction chamber having a substrate therein, the substrate having a surface;
flowing the supercritical fluid having the first precursor dispersed therein into the chamber to form a first component deposited over a surface of the substrate; and
flowing the second precursor into the chamber after the flowing the first precursor into the reaction chamber and separately in time from the flowing of the first precursor into the reaction chamber, the second precursor within the reaction chamber forming a second component deposited over the surface of the substrate, the first and second components together forming the material deposited over the substrate.
40. The method of claim 39 wherein the supercritical fluid having the first precursor dispersed therein is a first supercritical fluid; and wherein the second precursor is dispersed in a second supercritical fluid as the second precursor is flowed into the reaction chamber.
41. The method of claim 39 wherein the first precursor has a vapor pressure of less than or equal to about 0.1 Torr at 100\xb0 C.
42. The method of claim 39 wherein:
the first precursor comprises a metal;
the second precursor comprises nitrogen; and
the material deposited over the substrate comprises a nitride of the metal from the first precursor.
43. The method of claim 39 wherein:
the first precursor comprises a metal;
the second precursor comprises oxygen; and
the material deposited over the substrate comprises an oxide of the metal from the first precursor.
44. The method of claim 43 wherein the first precursor comprises hafnium, titanium or tantalum.
45. The method of claim 39 wherein one or more conditions within the reaction chamber are below critical conditions of the supercritical fluid at some time while the fluid is within the reaction chamber so that the supercritical fluid transforms to a non-supercritical state within the reaction chamber.
46. A method of forming a layer over a substrate, comprising:
providing a supercritical fluid comprising at least two different precursors dispersed therein;
providing a reaction chamber having a substrate therein, the substrate having a surface;
flowing the supercritical fluid into the reaction chamber and forming a first material comprising components of the at least two different precursors, the first material being formed over at least a portion of the surface of the substrate; after forming the first material, some of the at least two precursors remaining free in the chamber;
removing substantially all of the at least two precursors remaining free from within the chamber; and
after removing substantially all of the at least two precursors, flowing a reactant into the chamber to chemically convert at least some of the first material to a second material.
47. The method of claim 46 wherein one of the at least two different precursors comprises hafnium and another of the at least two different precursors comprises aluminum; and wherein the first material comprises hafnium from said one of the precursors and aluminum from said other of the precursors.
48. The method of claim 47 wherein the first material consists essentially of the hafnium and the aluminum.
49. The method of claim 46 wherein one of the at least two different precursors comprises titanium and another of the at least two different precursors comprises tantalum; and wherein the first material comprises titanium from said one of the precursors and tantalum from said other of the precursors.
50. The method of claim 49 wherein the reactant comprises oxygen, and wherein the chemical conversion of at least some of the first material comprises oxidation of at least some of the tantalum and titanium of the first material.
51. The method of claim 49 wherein the first material consists essentially of the titanium and the tantalum.
52. The method of claim 51 wherein the reactant comprises oxygen; and wherein the chemical conversion of at least some of the first material comprises oxidation of the tantalum and titanium of the first material to form the second material to consist of tantalum oxide and titanium oxide.
53. The method of claim 49 wherein said one of the precursors is TiF5 or titanium isopropoxide; and wherein said other of the precursors is pentakis(dimethylamino)tantalum, TaF5 or tantalum ethoxide.
54. The method of claim 49 wherein a ratio of said one of the precursors to said other of the precursors within the supercritical fluid is from about 5:95 to about 10:90.
55. The method of claim 49 wherein a ratio of titanium to tantalum within the first material is from about 5:95 to about 10:90.
56. The method of claim 46 wherein the reactant comprises oxygen, and wherein the chemical conversion of at least some of the first material comprises oxidation of the first material.
57. The method of claim 46 wherein one or more conditions within the reaction chamber are below critical conditions of the supercritical fluid at some time while the supercritical fluid is in the chamber so that the supercritical fluid transforms to a non-supercritical state within the reaction chamber.
58. The method of claim 57 wherein the one or more conditions within the reaction chamber which are below the critical conditions of the supercritical fluid include a pressure which is below the critical pressure of the supercritical fluid.
59. The method of claim 57 wherein the one or more conditions within the reaction chamber are below the critical conditions as the supercritical fluid is flowed into the chamber so that the supercritical fluid transforms to the non-supercritical state upon being flowed into the chamber.
60. The method of claim 57 wherein:
the supercritical fluid is flowed into the chamber in the supercritical state and under conditions suitable to maintain the supercritical fluid in the supercritical state; and
after the supercritical fluid is flowed into the reaction chamber, conditions within the reaction chamber are changed to reduce the one or more conditions within the reaction chamber to below the critical conditions of the supercritical fluid.
61. A method of forming a layer over a substrate, comprising:
providing a supercritical fluid comprising a titanium-containing composition and a tantalum-containing composition dispersed therein;
providing a reaction chamber having a substrate therein, the substrate having a surface; and
flowing the supercritical fluid into the reaction chamber and forming a material comprising titanium from the titanium-containing composition and tantalum from the tantalum-containing composition, the material being formed over at least a portion of the surface of the substrate.
62. The method of claim 61 further comprising exposing the material to oxygen to convert at least some of the tantalum in the material to tantalum oxide, and to convert at least some of the titanium in the material to titanium oxide.
63. The method of claim 62 wherein substantially all of the tantalum in the material is converted to tantalum oxide, and wherein substantially all of the titanium in the material is converted to titanium oxide.
64. The method of claim 61 further comprising flowing an oxygen-containing composition into the reaction chamber after forming the material, the oxygen-containing composition interacting with tantalum and titanium of the material to form tantalum oxide and titanium oxide.
65. The method of claim 64 wherein some free titanium-containing composition and free tantalum-containing composition remains within the chamber after forming the material, the method further comprising purging substantially all of the free titanium-containing composition and free tantalum-containing composition from within the chamber prior to the flowing of the oxygen-containing composition into the chamber.
66. The method of claim 61 wherein the supercritical fluid consists essentially of CO2, and wherein the compositions dispersed within the supercritical fluid consist of the titanium-containing composition and the tantalum-containing composition.
67. The method of claim 61 wherein a ratio of the titanium-containing composition to the tantalum-containing composition within the supercritical fluid is from about 5:95 to about 10:90.
68. The method of claim 61 wherein a ratio of the titanium-containing composition to the tantalum-containing composition within the material is from about 5:95 to about 10:90.
69. The method of claim 61 wherein the titanium-containing composition is TiF5 or titanium isopropoxide; and wherein the tantalum-containing composition is tantalum ethoxide, TaF5 or pentakis(dimethylamino)tantalum.
70. The method of claim 61 wherein one or more conditions within the reaction chamber are below critical conditions of the supercritical fluid at some time while the supercritical fluid is within the reaction chamber so that the supercritical fluid transforms to a non-supercritical state within the reaction chamber.
71. The method of claim 70 wherein the one or more conditions within the reaction chamber which are below the critical conditions of the supercritical fluid include a pressure which is below the critical pressure of the supercritical fluid.
72. The method of claim 70 wherein the one or more conditions within the reaction chamber are below the critical conditions as the supercritical fluid is flowed into the chamber so that the supercritical fluid transforms to the non-supercritical state upon being flowed into the chamber.
73. The method of claim 70 wherein:
the supercritical fluid is flowed into the chamber in the supercritical state and under conditions suitable to maintain the supercritical fluid in the supercritical state; and
after the supercritical fluid is flowed into the reaction chamber, conditions within the reaction chamber are changed to reduce the one or more conditions within the reaction chamber to below the critical conditions of the supercritical fluid.

The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.

1. A hinge assembly for a deployable mirror, the hinge assembly comprising:
a base;
a mirror segment base coupled to the base;
a mirror segment coupled to the mirror segment base by two bearings; and
at least one linear actuator secured to the base and capable of adjusting the mirror segment.
2. The hinge assembly of claim 1, further comprising at least two flexures configured to couple the mirror segment base to the base.
3. The hinge assembly of claim 2, wherein each flexure includes a first portion connected to the mirror segment base, a second portion connected to the base and a third portion connecting the first portion to the second portion.
4. The hinge assembly of claim 3, wherein each flexure is fabricated from metal material.
5. The hinge assembly of claim 2, wherein the at least one linear actuator includes a first linear actuator secured to the base and capable of adjusting the mirror segment, and second and third linear actuators secured to the base and configured to move the mirror segment base.
6. The hinge assembly of claim 5, wherein each of the first, second, and third linear actuators is an ultrahigh resolution micro linear actuator.
7. The hinge assembly of claim 1, wherein each bearing is fabricated from ceramic material.
8. The hinge assembly of claim 7, wherein each bearing has a maximum surface roughness of 0.5 Ra and a maximum deviation from spherical shape of 0.000003 inches.
9. A hinge assembly for a deployable mirror, the hinge assembly comprising:
a mirror segment base including a body having two inwardly facing first and second bearing seats formed therein;
a mirror segment including a outer, oppositely facing surfaces having outwardly facing third and fourth bearing seats formed therein; and
first and second bearings each fabricated from ceramic material having a maximum surface roughness of 0.5 Ra and a maximum deviation from spherical shape of 0.000003 inches,
wherein the first bearing is positioned between mating first and third bearing seats of the mirror segment base and the mirror segment, respectively, and the second bearing is positioned between mating second and fourth bearing seats of the mirror segment base and the mirror segment, respectively.
10. The hinge assembly of claim 9, further comprising a base, the mirror segment base being coupled to the base.
11. The hinge assembly of claim 10, further comprising a first linear actuator secured to the base and configured to adjust the mirror segment.
12. The hinge assembly of claim 11, further comprising at least two flexures configured to couple the mirror segment base to the base.
13. The hinge assembly of claim 12, wherein each flexure includes a first portion connected to the mirror segment base, a second portion connected to the base and a third portion connecting the first portion to the second portion.
14. The hinge assembly of claim 13, wherein each flexure is fabricated from metal material.
15. The hinge assembly of claim 11, further comprising second and third linear actuators secured to the base and configured to adjust the mirror segment base.
16. The hinge assembly of claim 15, wherein each of the first, second, and third linear actuators is an ultrahigh resolution micro linear actuator.
17. A hinge assembly for a deployable mirror, the hinge assembly comprising:
a base;
a mirror segment base coupled to the base;
a mirror segment coupled to the mirror segment base by two bearings; and
means for adjusting the mirror segment.
18. The hinge assembly of claim 17, further comprising a first linear actuator secured to the base, and at least two flexures configured to couple the mirror segment base to the base.
19. The hinge assembly of claim 18, wherein each flexure includes a first portion connected to the mirror segment base, a second portion connected to the base and a third portion connecting the first portion to the second portion.
20. The hinge assembly of claim 18, further comprising second and third linear actuators secured to the base and configured to adjust the mirror segment base.