1. A method for producing a moulded plastic product having an outer skin and in inner core, the method comprising the steps of: providing a mould having a mould cavity; forming an outer skin from a first plastic material on at least two opposed surfaces inside the mould cavity; forming an inner core from a second plastic material inside the mould cavity; and at least partially curing the plastic materials to form a moulding inside the mould cavity via the application of heat, the method being characterised by the subsequent steps of simultaneously cooling the moulding and compressing the moulding so as to reduce its size in at least one dimension to a desired dimension of the finished product.
2. A method according to claim 1, wherein the moulding is removed from said mould cavity prior to the simultaneous steps of cooling and compressing.
3. A method according to claim 2, wherein said simultaneous steps of cooling and compressing are performed in a press having a cooling arrangement configured to cool the moulding whilst in the press.
4. A method according to claim 1, wherein the cooling step is effective to reduce the temperature of the moulding from over 200\xb0 C. to under 40\xb0 C.
5. A method according to claim 1, wherein the compressing step is effective to reduce said dimension by at least 20%.
6. A method according to claim 1, wherein the compressing step comprises applying a pressure of at least 150 Ncm2 to the moulding for the duration of the cooling step.
7. A method according to claim 1, wherein said step of forming the outer skin comprises filling the mould cavity with said first plastic material in particulate form, heating the mould to form a skin of melted particulate against said at least two opposed mould surfaces, and removing un-melted particulate from the mould cavity once a desired thickness of skin has been formed on said surfaces.
8. A method according to claim 7, wherein said step of removing un-melted particulate from the mould cavity is performed by opening an outlet aperture formed in a lower part of the mould, and permitting the un-melted particulate material to fall through the outlet aperture under gravity or by turning the mould to pour out the un-melted material.
9. A method according to claim 8, wherein said outlet aperture is subsequently closed after removal of the un-melted particulate material, ready for the receipt of said second plastic material in the mould cavity.
10. A method according to claim 7, wherein said step of filling the mould cavity with said first plastic material involves pouring said material in particulate form through an inlet aperture formed in an upper part of the mould, and subsequently closing said inlet aperture.
11. A method according to claim 1, wherein said step of forming the inner core comprises filling the mould cavity with said second plastic material in particulate form after the formation of the outer skin on said at least two opposed surfaces, and heating the mould to at least partially cure substantially the entire volume of said second material inside the mould cavity.
12. A method according to claim 11, wherein said step of filling the mould cavity with said second plastic material involves pouring said material in particulate form through an inlet aperture formed in an upper part of the mould, and subsequently closing said inlet aperture.
13. A method according to claim 11, wherein the mould is held at an internal temperature of at least 200\xb0 C. for a period of at least 5 minutes.
14. A method according to claim 1, wherein at least one of said first and second materials comprises recycled High Impact Polystyrene (HIPS).
15. A method according to claim 1, wherein the second material comprises recycled polyethylene.
The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.
1. A system for verifying accuracy of a raster scanned image of a document comprising:
an input tray that holds documents prior to imaging;
an input imaging device that captures an image of an unaltered document in the input tray;
an image processor configured to receive the captured image of the unaltered document in the input tray;
a document transport system configured to transport the unaltered document through a document scanner;
a raster capture device for capturing a raster scanned image of the unaltered document, wherein the raster scanned image is transmitted to the image processor;
wherein the image processor is configured to verify the accuracy of the raster scanned image by comparing the raster scanned image of the unaltered document to the captured input tray image of the unaltered document; and
wherein the image processor is further configured to modify scanner functions if the raster scanned image of the unaltered document does not match the captured input tray image of the unaltered document.
2. The system as in claim 1 wherein the scanner functions are selected from a group consisting of rotation of the raster capture device, changing a color capture mode, or cleaning image optics.
3. The system as in claim 1 wherein the input tray image of the unaltered document is captured as an area image.
4. The system as in claim 1 wherein the input tray image of the unaltered document is low resolution.
5. The system as in claim 1 wherein the input tray image of the unaltered document is high resolution.
6. The system as in claim 1, wherein the image processor is configured to alert a document scanner operator if the raster scanned image of the document does not match the input tray image of a document.
7. The system as in claim 1 further comprising:
an output tray for holding documents after the documents exit the scanner;
wherein the image processor is configured to receive the image; and
wherein the image processor is configured to verify the accuracy of the raster scanned image by comparing the raster scanned image of the document to the input tray image of the unaltered document or the output tray image of the document or both.