1. A solid composition that exhibits catalytic activity for ammoxidation or oxidation of propane and iso-butane in the gaseous phase, which comprises one or more crystalline phases at least one of which is a first phase characterized as having the M1 crystalline structure, wherein said first phase has a unit cell volume in a range upward from 2250 A3 to about 2350 A3, a first crystallite dimension and a transverse thereto a second dimension with the proviso that the ratio of first to second dimensions is in a range downward from about 2.5 to about 0.7; and wherein at least a portion of the composition is formed under conditions of crystallization by combining sources of metal ions in amounts consistent with a nominal mixed oxide material represented by the empirical formula:
MoVaSbbNbcO\u03b4
Where 0.1<a<1.0,
0.01<b<1.0,
0.001\u2266c\u22660.25, and
\u03b4 is the number of oxygen atoms required to maintain electro-neutrality of the other component elements present.
2. The solid composition of claim 1 wherein at least a portion of the crystalline material is formed by a process which comprises combining the sources of metal ions in aqueous solutions, drying the resulting combined mixture to recover solid materials, and maintaining the recovered solids at elevated temperatures for times sufficient to form at least the first crystalline phase.
3. The composition of claim 1 wherein the first phase is characterized as having the M1 crystalline structure that has a unit cell volume in a range upward from 2255 A3 to about 2290 A3, a major dimension and transverse thereto a second dimension with the proviso that the ratio of major to transverse dimensions is in a range downward from about 1.75 to about 0.7.
4. The composition of claim 1 further comprising tellurium (Te).
5. A solid composition that exhibits catalytic activity for ammoxidation or oxidation of propane and iso-butane in the gaseous phase, which comprises one or more crystalline phases at least one of which is a first phase characterized as having the M1 crystalline structure, wherein said first phase has a unit cell volume in a range upward from 2250 A3 to about 2350 A3, a first crystallite dimension and a transverse thereto a second dimension with the proviso that the ratio of first to second dimensions is in a range downward from about 2.5 to about 0.7; and wherein at least a portion of the composition is formed under conditions of crystallization by combining sources of metal ions in amounts consistent with a nominal mixed oxide material represented by the empirical formula:
MoVaSbbNbcXdAfO\u03b4
Where
X is selected from the group consisting of Ti, Sn, Ge, Zr, Hf; and mixtures thereof,
A is selected from the group consisting of Ce, Nd and mixtures thereof,
0.1<a<1.0,
0.01<b<0.5,
0.001<c<0.25,
0.005<d<0.4,
0\u2266f<0.1, and
\u03b4 is the number of oxygen atoms required to maintain electro-neutrality of the other component elements present with the proviso that one or more of the other elements in the mixed oxide can be present in an oxidation state lower than its highest oxidation state.
6. The composition of claim 5 wherein the first phase is characterized as having the M1 crystalline structure that has a unit cell volume in a range upward from 2255 A3 to about 2290 A3, a first dimension and transverse thereto a second dimension with the proviso that the first of major to second dimensions is in a range downward from about 1.75 to about 1.0.
7. The solid composition of claim 5 wherein at least a portion of the crystalline material is formed by a process which comprises combining the sources of metal ions in aqueous solutions or aqueous mixtures, drying the resulting aqueous mixture to recover solid materials, and maintaining the recovered solids at elevated temperatures for times sufficient to form at least the first crystalline phase.
8. The composition of claim 5 wherein the aqueous mixtures are reacted at temperatures below about 100\xb0 C. and ambient, or near ambient, pressure, and the recovered solid materials are first maintained at elevated temperatures of no more than about 400\xb0 C., and thereafter in a range upward from about 550\xb0 C. to 700\xb0 C. and ambient, or near ambient, pressure.
9. The solid composition of claim 5 wherein at least a portion of the crystalline material is formed by a process which comprises combining the sources of metal ions in aqueous solutions or aqueous mixtures, maintaining the resulting aqueous mixture at elevated temperatures and pressures for times sufficient to form at least the first crystalline phase.
10. The composition of claim 5 wherein the composition that exhibits catalytic activity for ammoxidation of propane in the gaseous phase comprises a mixed metal oxide in particulate form comprising, as component elements, molybdenum (Mo), vanadium (V), antimony (Sb) titanium (Ti), and niobium (Nb).
11. The catalyst composition of claim 5 wherein the composition that exhibits catalytic activity for ammoxidation of propane in the gaseous phase comprises a mixed metal oxide in particulate form having, as component elements, molybdenum (Mo), vanadium (V), antimony (Sb) niobium (Nb), titanium (Ti), and cerium (Ce).
12. A solid composition that exhibits catalytic activity for ammoxidation or oxidation of propane and iso-butane in the gaseous phase, which comprises one or more crystalline phases at least one of which is a first phase characterized as having the M1 crystalline structure, wherein said first phase has a unit cell volume in a range upward from 2250 A3 to about 2350 A3, a first crystallite dimension and a transverse thereto a second dimension with the proviso that the ratio of first to second dimensions is in a range downward from about 2.5 to about 0.7; and wherein at least a portion of the composition is formed under conditions of crystallization by combining sources of metal ions in amounts consistent with a nominal mixed oxide material represented by the empirical formula:
MoVaSbbNbeTidO\u03b4
Where
0.1<a<1.0,
0.01<b<1.0,
0.01<c<0.25,
0.005<d<0.4, and
\u03b4 is the number of oxygen atoms required to maintain electro-neutrality of the other component elements present.
The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.
1. A peripheral component for audio equipment comprising: a polyphenylene ether-based resin (A); a polystyrene-based resin (B); and a polyolefin-based resin (C), wherein the polyolefin-based resin comprises at least one selected from the group consisting of polyethylene, polypropylene, and an ethylenepropylene copolymer, and wherein the peripheral component is used for at least one member selected from the group consisting of a horn, a field cover, an equalizer, an equalizer support, and a speaker front mounting plate.
2. A peripheral component for audio equipment according to claim 1, wherein a weight ratio of the polyphenylene ether-based resin (A) to the polystyrene-based resin (B) (A)(B) is 9010 to 7030.
3. A peripheral component for audio equipment according to claim 1 wherein the polyolefin-based resin (C) is included in an amount of 5 to 20 parts by weight with respect to 100 parts by weight in total of the polyphenylene ether-based resin (A) and the polystyrene-based resin (B).
4. A peripheral component for audio equipment according to claim 1 wherein the polyphenylene ether-based resin (A) and the polystyrene-based resin (B) are alloyed.
5. A peripheral component for audio equipment according to claim 1 wherein the polyphenylene ether-based resin has a number average molecular weight of 5,000 to 1,000,000.
6. A peripheral component for audio equipment according to claim 1 wherein the polystyrene-based resin has a number average molecular weight of 400 to 500,000.
7. A peripheral component for audio equipment according to claim 1, wherein the polyolefin-based resin has a number average molecular weight of 500 to 100,000.
8. A speaker comprising the peripheral component for audio equipment according to claim 1.