1461082776-7605b3d0-49ef-44a6-9352-fa612b15a004

1. A composite of mixed metal oxides comprising:
a ceria-zirconia solid solution that optionally further comprises at least one rare earth oxide other than ceria; and
alumina in an amount in the range of 1 to less than 30% by weight of the composite;
wherein the mixed metal oxide composite, after 12 hours of hydrothermal aging at 1050\xb0 C., has a reducibility of ceria of at least 50% in H2-TPR at a temperature up to 900\xb0 C.
2. The composite of mixed metal oxides of claim 1, wherein the alumina formed by using a colloidal alumina precursor.
3. The composite of mixed metal oxides of claim 1, wherein the alumina content is in the range of 5 to less than 20% by weight of the composite.
4. The composite of mixed metal oxides of claim 3, wherein the alumina content is in the range of 10 to 18% by weight of the composite.
5. The composite of mixed metal oxides of claim 1, wherein the cumulative pore volume is at least 0.75 mlg after 12 hours of hydrothermal aging at 1050\xb0 C.
6. The composite of mixed metal oxides of claim 1, wherein the pore volume in the pore radius range of 30 to 1000 \u212b is 35 vol. % or more of the cumulative total pore volume after 12 hours of hydrothermal aging at 1050\xb0 C.
7. The composite of mixed metal oxides of claim 1, wherein the surface area is greater than 24 m2g after 12 hours of hydrothermal aging at 1050\xb0 C.
8. The composite of mixed metal oxides of claim 1, wherein the surface area is in the range of 24 m2g to 80 m2g after 12 hours of hydrothermal aging at 1050\xb0 C.
9. The composite of mixed metal oxides of claim 1, wherein the H2 consumption in H2-TPR at a temperature of up to 900\xb0 C. is 7 mlg or greater.
10. The composite of mixed metal oxides of claim 1, wherein the phase of the ceria-zirconia solid solution is cubic, tetragonal, or a combination thereof.
11. The composite of mixed metal oxides of claim 1 comprising, by weight of the composite:
alumina in the range of 5% to less than 20%;
ceria in the range of 1% to 50%;
zirconia in the range of 10% to 70% by weight;
rare earth oxides other than ceria in the range of 0% to 20%.
12. The composite of mixed metal oxides of claim 12 comprising by weight of the composite:
alumina in the range of 10% to 18%;
ceria in the range of 5% to 40%;
zirconia in the range of 10% to 60% by weight;
a rare earth oxide other than ceria in the range of 1% to 15%.
13. The composite of claim 1 comprising at least one rare earth oxide selected from the group consisting of yttria, praseodymia, lanthana, neodymia, samaria, and gadolinia.
14. A method of making a composite of mixed metal oxides comprising ceria, zirconia, and alumina, the method comprising:
forming an aqueous solution comprising a cerium salt, a zirconium salt, and optionally at least one rare earth metal salt other than cerium compound;
providing a source of alumina in an amount that results in an alumina content in the range of 1 to less than 30% by weight in the composite;
mixing the aqueous solution and the source of alumina to form a mixture;
adjusting the pH of the mixture with a basic agent to form a raw precipitate;
isolating the raw precipitate to obtain an isolated precipitate; and
calcining the isolated precipitate at a temperature of at least 600\xb0 C. to form the composite of mixed metal oxides.
15. The method of claim 14, wherein the source of alumina is a suspension of colloidal alumina.
16. The method of claim 14, further comprising hydrothermally treating the raw precipitate at a temperature of at least 80\xb0 C.
17. The method of claim 14, further comprising treating the raw precipitate with an anionic surfactant, a cationic surfactant, a zwitterionic surfactant, a non-ionic surfactant, a polymeric surfactant, or combinations thereof.
18. The method of claim 14, wherein the step of hydrothermally treating the raw precipitate is at a temperature of at least 100\xb0 C., and further comprising the step of treating the raw precipitate with an anionic surfactant, a cationic surfactant, a zwitterionic surfactant, a non-ionic surfactant, a polymeric surfactant, or combinations thereof.
19. A catalyst for treating engine exhaust comprising a catalytic material coated on a substrate, the catalytic material comprising:
the composite of mixed metal oxide of claim 1 which is used as oxygen storage component or a precious metal support, and
a precious metal component selected from the group consisting of palladium, rhodium, platinum, and combinations thereof.
20. The catalyst of claim 19 comprising the composite of mixed metal oxides in the range of about 0.1 gin3 to about 3.5 gin3.
21. The catalyst of claim 19, wherein the catalyst is a three-way conversion catalyst and the catalytic material is effective to substantially simultaneously oxidize hydrocarbons and carbon monoxide and reduce nitrogen oxides.
22. The catalyst of claim 19, wherein the catalyst is a diesel oxidation catalyst and the catalytic material is effective to substantially simultaneously oxidize hydrocarbons and carbon monoxide.
23. An emissions after-treatment system for treating an exhaust stream from an engine comprising the catalyst of claim 19 in flow communication with the exhaust stream.
24. A method of treating an exhaust stream comprising passing the exhaust stream through the catalyst of claim 19.

The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.

1. A process to prepare an olefin polymerization catalyst, said process comprising:
(a) in a diluent, combining a diorganomagnesium compound of the formula MgRaRb with a first source of chloride to give a first product mixture, wherein the molar ratio of chloride in said first source of chloride to magnesium Mg is from 1.5:1 to 1.95:1 and where Ra and Rb are individually C1 to C8 hydrocarbyl groups;
(b) without isolating any solids present in said first product mixture, combining said first product mixture with a second source of chloride to give a second product mixture, wherein the molar ratio of chloride in said second source of chloride to total magnesium Mg is from 0.01:1 to 0.7:1;
wherein the total molar ratio of chloride from said first source of chloride and from said second source of chloride to magnesium Mg does not exceed a ratio of 2.2:1;
(c) without isolating any solids present in said second product mixture, combining said second product mixture with a titanium species to give a third product mixture, said titanium species having the formula TiCln(OR)m, wherein n is from 2 to 4, n+m=4 and OR is selected from an alkoxy group, an aryloxy group, or mixtures thereof; and
(d) i) combining said third product mixture with an activator; or
ii) combining solids isolated from said third product mixture with an activator.
2. The process of claim 1 wherein the total molar ratio of chloride from said first source of chloride and from said second source of chloride to magnesium Mg does not exceed a ratio of 2.1:1.
3. The process of claim 1 wherein the molar ratio of chloride in said first source of chloride to magnesium Mg is from 1.65:1 to 1.95:1.
4. The process of claim 3 wherein the molar ratio of chloride in said second source of chloride to total magnesium Mg is from 0.015:1 to 0.4:1.
5. The process of claim 1, with the proviso that electron donors are not added.
6. The process of claim 1 wherein the molar ratio of Mg:Ti is from 3:1 to 15:1.
7. The process of claim 1 wherein said titanium species is TiCl4.
8. The process of claim 1 wherein said activator has the formula AlR4x(OR5)y wherein x is from 1 to 3, x+y=3, R4 is a C1 to C10 hydrocarbyl group and R5 is an alkyl or an aryl group.
9. The process of claim 8 wherein the molar ratio Al:Ti is from 0.5:1 to 50:1.
10. The process of claim 1 wherein said first source of chloride and said second source of chloride are the same compound.
11. An olefin polymerization process comprising contacting one or more olefins with the olefin polymerization catalyst prepared according to the process of claims 1.
12. A solution phase polymerization process in which ethylene and at least one comonomer are contacted with the olefin polymerization catalyst prepared according to the process of claims 1.
13. A solution phase polymerization process catalyzed by an olefin polymerization catalyst, said catalyst being prepared in-line by a process comprising:
(a) forming a first product mixture by combining a diorganomagnesium compound and a first source of chloride, in a diluent, wherein the molar ratio of chloride in said first source of chloride to said diorganomagnesium compound is from 1.5:1 to 1.95:1;
(b) forming a second product mixture by combining said first product mixture with a second source of chloride, wherein the molar ratio of chloride in said second source of chloride to said diorganomagnesium compound is from 0.01:1 to 0.7:1;
provided that the total molar ratio of chloride from said first source of chloride and from said second source of chloride to magnesium Mg does not exceed a ratio of 2.2:1;
(c) forming a third product mixture by combining said second product mixture with a titanium species of the formula TiCln(OR)m, wherein n is from 2 to 4, n+m=4 and OR is selected from an alkoxy group, an aryloxy group, or mixtures thereof;
(d) combining said third product mixture with an activator.
14. The process of claim 13 wherein (a)-(c) are carried out upstream of a polymerization zone.
15. The process of claim 13 wherein (a)-(d) are carried out upstream of a polymerization zone.
16. The process of claim 13 wherein the total molar ratio of chloride from said first source of chloride and from said second source of chloride to magnesium Mg does not exceed a ratio of 2.1:1.
17. The process of claim 13 wherein the molar ratio of chloride in said first source of chloride to magnesium Mg is from 1.65:1 to 1.95:1.
18. The process of claim 17 wherein the molar ratio of chloride in said second source of chloride to total magnesium Mg is from 0.015:1 to 0.4:1.
19. The process of claim 13 with the proviso that electron donors are not added.
20. The process of claim 13 wherein the molar ratio of Mg:Ti is from 3:1 to 15:1.
21. The process of claim 13 wherein said titanium species is TiCl4.
22. The process of claim 13 wherein said activator has the formula AlR4x(OR5)y wherein x is from 1 to 3, x+y=3, R4 is a C1 to C10 hydrocarbyl group and R5 is an alkyl or an aryl group.
23. The process of claim 22 wherein the molar ratio Al:Ti is from 0.5:1 to 50:1.
24. The process of claim 13 wherein said first source of chloride and said second source of chloride are the same compound.
25. The process of claim 13 wherein said diorganomagnesium compound has the formula MgRaRb, wherein Ra and Rb are individually C1 to C8 hydrocarbyl groups.
26. A process to prepare an olefin polymerization catalyst, said process comprising:
(a) forming a solid product by combining in a diluent, a diorganomagnesium compound of the formula MgRaRb with a source of chloride wherein the molar ratio of chloride provided by said source of chloride to magnesium Mg is from 1.55:1 to 2.2:1 and where Ra and Rb are individually C1 to C8 hydrocarbyl groups; wherein
i) from 70 to 99.5 mol % of said source of chloride is combined with MgRaRb in a first contacting stage; and
ii) the balance of said source of chloride is combined with MgRaRb in a second contacting stage;
provided that the molar ratio of chloride provided by said source of chloride to magnesium Mg in said first contacting stage does not exceed 2:1;

(b) without isolating said solid product, adding a titanium species, said titanium species having the formula TiCln(OR)m, wherein n is from 2 to 4, n+m=4 and OR is selected from an alkoxy group, an aryloxy group, or mixtures thereof; and
(c) adding an activator.
27. The process according to claim 26, wherein from 75 to 90 mol % of said source of chloride is combined with MgRaRb in a first contacting stage and the balance of said source of chloride is combined with MgRaRb in a second contacting stage.