1. A method for manufacturing a semiconductor device with a bump electrode, the bump electrode including a resin material as a core and having at least a top surface covered with a conductive film, the method comprising:
placing the resin material on a substrate on which an electrode terminal is formed, the resin material being placed by an inkjet method;
drying the resin material; and
forming an interconnecting metal that connects the electrode terminal to the top surface of the resin material, wherein:
the placing of the resin material and the drying of the resin material are repeated.
2. The method for manufacturing a semiconductor device according to claim 1, wherein the resin material is placed by dropping a plurality of droplets from a discharger.
3. The method of manufacturing a semiconductor device according to claim 2, wherein the discharger has a plurality of nozzles for discharging droplets.
4. The method of manufacturing a semiconductor device according to claim 1, further comprising processing at least part of an area of a surface of the substrate to be lyophobic to the resin material before placing the resin material.
5. The method of manufacturing a semiconductor device according to claim 1, wherein a resin projection extending linearly at approximately a uniform height is formed on the substrate by placing the resin material.
6. The method of manufacturing a semiconductor device according to claim 1, wherein a plurality of resin projections aligned approximately on one straight line is formed on the substrate by placing the resin material.
7. The method of manufacturing a semiconductor device according to claim 1, wherein the interconnecting metal is formed by using an inkjet method.
8. The method of manufacturing a semiconductor device according to claim 7, wherein placing a droplet containing a material for forming the interconnecting metal at every certain distance on the substrate is repeated while shifting a starting position to place the droplet.
9. A semiconductor device manufactured by using the method of manufacturing a semiconductor device according to claim 1.
10. A circuit board on which the semiconductor device according to claim 9 is mounted.
11. An electro-optic device having the circuit board according to claim 10.
12. An electronic apparatus having the electro-optic device according to claim 11.
13. A method of manufacturing a semiconductor device with a bump electrode comprising:
providing a substrate on which an electrode terminal is formed;
disposing a resin material on the substrate by an inkjet method;
drying the resin material; and
connecting the electrode terminal to a top surface of the resin material with an interconnecting metal such that the bump electrode is formed with the resin material as a core and a conductive film covering at least a top surface of the resin material, wherein:
the disposing of the resin material and the drying of the resin material are repeated.
14. A method for manufacturing a semiconductor device with a bump electrode, the bump electrode including a resin material as a core and having at least a top surface covered with a conductive film, the method comprising:
placing the resin material on a substrate on which an electrode terminal is formed, the resin material being placed by an inkjet method; and
forming an interconnecting metal that connects the electrode terminal to the top surface of the resin material, wherein the interconnecting metal is formed by using an inkjet method, and wherein placing a droplet containing a material for forming the interconnecting metal at every certain distance on the substrate is repeated while shifting a starting position to place the droplet.

The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.

1. A mine opening lined with a liner comprising the product of reaction of:
(a) a hydrophilic prepolymer bearing isocyanate groups that are capable of reacting with water to form a gelled mass; and
(b) a water-borne polymer dispersion, said polymer bearing groups that are reactive to said isocyanate groups.
2. A mine opening lined with a liner comprising the product of reaction of:
(a) a hydrophilic prepolymer bearing isocyanate groups that are capable of reacting with water to form a gelled mass; and
(b) a water-borne polymer dispersion, said polymer bearing groups that are reactive to said isocyanate groups;
wherein said dispersion has a sufficiently high solids content, and said polymer has a sufficiently high modulus and glass transition or crystalline melting temperature, that said product of reaction exhibits a 24-hour Tensile Strength of at least about 2.5 MPa.
3. A mine opening lined with a liner comprising the product of reaction of:
(a) a hydrophilic prepolymer bearing isocyanate groups; and
(b) a water-borne polyurethane-polyacrylic or poly(styrene-acrylic) dispersion, said polyurethane-polyacrylic or poly(styrene-acrylic) bearing groups that are reactive to said isocyanate groups.
4. A mine opening lined with a liner comprising the product of reaction of:
(a) a hydrophilic prepolymer bearing isocyanate groups that are capable of reacting with water to form a gelled mass; and
(b) a water-borne polymer dispersion, said polymer bearing groups that are reactive to said isocyanate groups;

wherein said dispersion has a water content no greater than about 80 percent by weight, based upon the total weight of said dispersion.
5. A kit for producing a liner, said kit comprising
(a) a hydrophilic prepolymer bearing isocyanate groups that are capable of reacting with water to form a gelled mass; and
(b) a water-borne polymer dispersion which when combined with said component (a) reacts to form a liner, said polymer bearing groups that are reactive to said isocyanate groups;
wherein said dispersion has a sufficiently high solids content, and said polymer has a sufficiently high modulus and glass transition or crystalline melting temperature, that said liner exhibits a 24-hour Tensile Strength of at least about 2.5 MPa.
6. A kit according to claim 5, wherein said polymer used in component (b) has a molecular weight in the range of at least about 50,000.
7. A kit according to claim 5, wherein said polymer of component (b) is in the form of particles of a size from about 10 to about 10,000 nm.
8. A kit according to claim 5, wherein said dispersion has a solids content of at least about 30 percent by weight, based upon the total weight of said dispersion.
9. A kit according to claim 5, wherein a film prepared from said polymer used in component (b) has a tensile modulus of at least about 6.89 MPa at 100% elongation.
10. A kit according to claim 5, wherein a film prepared from said polymer used in component (b) has a value of Tg or Tm greater than about 30\xb0 C.
11. A kit according to claim 5, wherein said dispersion contains no co-solvent.
12. A kit according to claim 5, wherein said liner exhibits a 4-hour Tensile Strength of at least about 1 MPa.
13. A kit according to claim 5, wherein said prepolymer is formed by reacting a polymer bearing hydroxyl groups with a monomeric polyisocyanate to form a urethane-containing polymer bearing isocyanate groups, which is purified by removing unreacted monomeric polyisocyanate or by quenching unreacted monomeric polyisocyanate with a compound that is reactive to isocyanate groups.
14. A kit according to claim 5, wherein said polymer dispersion is selected from the group consisting of polyurethane dispersions and poly(styrene-acrylic) dispersions.
15. A kit according to claim 14, wherein said polymer dispersion is a polyurethane dispersion.
16. A kit according to claim 15, wherein said polyurethane dispersion is a polyurethane-polyacrylic dispersion.
17. A kit according to claim 5, wherein said polymer dispersion is in admixture with a dispersion of an acrylic polymer, a styrene-butadiene copolymer, or a vinyl acetate polymer.
18. A kit according to claim 5, wherein the weight ratio of component (a) to component (b) is in the range of about 1:3 to about 1:10.
19. The kit of claim 5, wherein said liner has a thickness in the range of from about 0.5 mm to about 6 mm.
20. The kit of claim 5, wherein said prepolymer is derived from at least one polyether polyol.
21. The kit of claim 20, wherein said polyether polyol is trifunctional.
22. The kit of claim 5, wherein said groups that are reactive to said isocyanate groups are amino groups.
23. A kit for producing a liner, said kit comprising
(a) a hydrophilic prepolymer bearing isocyanate groups; and
(b) a water-borne polyurethane-polyacrylic or poly(styrene-acrylic) dispersion which when combined with said component (a) reacts to form a liner, said polyurethane-polyacrylic or poly(styrene-acrylic) bearing groups that are reactive to said isocyanate groups.
24. A kit according to claim 23, wherein said kit further comprises expandable graphite.
25. A kit according to claim 23, wherein said prepolymer is derived from at least one polyether polyol and said isocyanate groups are derived from at least one aromatic polyisocyanate.
26. A kit according to claim 23, wherein said dispersion is a polyurethane-polyacrylic dispersion.
27. A kit for producing a liner, said kit comprising
(a) a hydrophilic prepolymer bearing isocyanate groups that are capable of reacting with water to form a gelled mass; and
(b) a water-borne polymer dispersion which when combined with said component (a) reacts to form a liner, said polymer bearing groups that are reactive to said isocyanate groups;

wherein said dispersion has a water content no greater than about 80 percent by weight, based upon the total weight of said dispersion.
28. A kit for producing a liner, said kit comprising
(a) a hydrophilic prepolymer bearing isocyanate groups that are capable of reacting with water to form a gelled mass; and
(b) a water-borne polymer dispersion which when combined with said component (a) reacts to form a liner, said polymer bearing groups that are reactive to said isocyanate groups;
wherein said dispersion has a sufficiently high solids content, and said polymer has a sufficiently high modulus and glass transition or crystalline melting temperature, that said liner exhibits a 4-hour Tensile Strength of at least about 1 MPa.