1461097367-7489c50a-6615-4eb2-a682-e0eaf8abe328

1. A method of making a vehicle floor covering, comprising:
providing a mold having a forming surface;
spraying a polyurethane composition toward the forming surface to form a polyurethane top layer of the floor covering;
partially curing the polyurethane layer to form a solid polyurethane top layer;
spraying a filled mass composition onto the polyurethane top layer before the solid polyurethane top layer is fully cured to form a mass layer, wherein the mass layer does not fully penetrate the solid polyurethane top layer;
curing the polyurethane top layer and mass layer to form the vehicle floor covering in the mold; and
removing the vehicle floor covering from the mold.
2. The method of claim 1 further comprising:
adding a decoupler next to the mass layer in the mold before removing the vehicle floor covering from the mold.
3. The method of claim 2, wherein the step of adding the decoupler is performed by pouring a foam polyurethane composition onto the mass layer.
4. The method of claim 2, wherein the step of adding the decoupler is performed by inserting a sheet form decoupler into the mold and onto the mass layer.
5. The method of claim 2, wherein the step of adding the decoupler is performed by inserting lightweight polyester batting into the mold and onto the mass layer.
6. The method of claim 1, wherein the step of spraying the mass layer further comprising:
spraying the filled mass composition at a plurality of different thicknesses in specified areas of the mold to form a mass layer having greater thickness in some specified areas than in other areas.
7. The method of claim 1, wherein no adhesive is applied between the solid polyurethane top layer and the mass layer and the inherent properties of the solid polyurethane top layer and the mass layer are utilized to bond these two layers together.
8. The method of claim 1, wherein the polyurethane top layer is a reaction injection molding composition.
9. The method of claim 1, wherein the filled mass composition is filled ethyl vinyl acetate.
10. The method of claim 1, further comprising trimming the outer edge of the floor covering after the floor covering is removed from the mold.
11. A vehicle floor covering, comprising:
a polyurethane top layer having a top side and a bottom side; and
a filled mass composition attached to the polyurethane top layer with the filled mass composition being partially disposed in the polyurethane top layer, wherein the mass layer penetrates the bottom side but does penetrate the solid polyurethane top layer to the top side.
12. The vehicle floor covering of claim 11, further comprising a decoupler attached to the mass layer on the opposite side of the filled mass layer from the polyurethane top layer.
13. The vehicle floor covering of claim 12 wherein the decoupler is a poured foam composition.
14. The vehicle floor covering of claim 12 wherein the decoupler is a lightweight polyester batting.
15. The vehicle floor covering of claim 12 wherein the polyurethane top layer is a reaction injection molding composition.
16. The vehicle floor covering of claim 12, wherein the filled mass composition is filled ethyl vinyl acetate.

The claims below are in addition to those above.
All refrences to claim(s) which appear below refer to the numbering after this setence.

1. A paper coating or binding formulation, comprising:
an aqueous polymer dispersion comprising a copolymer derived from 40% to 75% by weight of styrene, 25% to 60% by weight of butadiene, 1% to 10% by weight of itaconic andor (meth)acrylic acid, 0% to 3% by weight of (meth)acrylamide, 0% to 20% by weight of (meth)acrylonitrile, and greater than 0% to less than 50% by weight of a carbohydrate-derived compound having a dextrose equivalent (DE) of about 10 to about 35, based on the total monomer weight; and
a tetrasulfonate-based fluorescent whitening agent.
2. The formulation according to claim 1, wherein the carbohydrate-derived compound is selected from the group consisting of dextrins, maltodextrins, and mixtures thereof.
3. The formulation according to claim 1, wherein the DE of the carbohydrate-derived compound is from about 12.5 to about 25.
4. The formulation according to claim 1, wherein the DE of the carbohydrate-derived compound is from about 15 to about 20.
5. The formulation according to claim 1, wherein the weight average molecular weight of the carbohydrate-derived compound is from about 3,000 to about 20,000.
6. The formulation according to claim 1, wherein the weight average molecular weight of the carbohydrate-derived compound is from about 5,000 to about 17,000.
7. The formulation according to claim 1, wherein the carbohydrate-derived compound is soluble in water at room temperature in an amount of greater than about 40% by weight.
8-10. (canceled)
11. The formulation according to claim 1, wherein the copolymer is derived from about 5 to about 45 percent by weight of the carbohydrate-derived compound based on the total monomer weight.
12. The formulation according to claim 1, wherein the copolymer is derived from about 8 to about 40 percent by weight of the carbohydrate-derived compound based on the total monomer weight.
13. The formulation according to claim 1, wherein the aqueous polymer dispersion comprises a disperse phase and an aqueous phase and the carbohydrate-derived compound provided in the copolymer is present in the disperse phase.
14. The formulation according to claim 1, wherein said fluorescent whitening agent is not activated.
15. The formulation according to claim 1, wherein the formulation is substantially free of polyvinyl alcohol, carboxymethylcellulose, polyvinylpyrrolidone, and water-insoluble starches.
16. The formulation according to claim 1, wherein the aqueous polymer dispersion further comprises a hexasulfonate-based fluorescent whitening agent.
17. A method of preparing a paper coating or binding formulation, comprising:
polymerizing a mixture of 40% to 75% by weight of styrene, 25% to 60% by weight of butadiene, 1% to 10% by weight of itaconic andor (meth)acrylic acid, 0% to 3% by weight of (meth)acrylamide, 0% to 20% by weight (meth)acrylonitrile, and greater than 0% to less than 50% by weight of a carbohydrate-derived compound having a dextrose equivalent (DE) of about 10 to about 35, based on the total monomer weight, in an aqueous medium to produce a styrene-butadiene copolymer in an aqueous polymer dispersion, and
mixing the aqueous polymer dispersion with a tetrasulfonate-based fluorescent whitening agent.
18. The method according to claim 17, wherein the carbohydrate-derived compound is selected from the group consisting of dextrins, maltodextrins, and mixtures thereof.
19. The method according to claim 17, wherein the DE of the carbohydrate-derived compound is from about 12.5 to about 25.
20. The method according to claim 17, wherein the weight average molecular weight of the carbohydrate-derived compound is from about 3,000 to about 20,000.
21. The method according to claim 17, wherein said polymerizing step comprising first mixing an aqueous solution of a carbohydrate-derived compound at room temperature comprising greater than about 40% by weight of the carbohydrate-derived compound with the styrene, butadiene, and itaconic andor (meth)acrylic acid and polymerizing the mixture to form the copolymer.
22. The method according to claim 17, wherein the copolymer is derived from about 5 to about 45 percent by weight of the carbohydrate-derived compound based on the total monomer weight.
23. The method according to claim 17, wherein said fluorescent whitening agent is not activated.
24. The method according to claim 17, wherein the formulation is substantially free of polyvinyl alcohol, carboxymethylcellulose, polyvinylpyrrolidone, and water-insoluble starches.
25. A method of improving the whitening properties of paper;
comprising:
providing an aqueous polymer dispersion comprising a copolymer derived from 40% to 75% by weight of styrene, 25% to 60% by weight of butadiene, 1% to 10% by weight of itaconic andor (meth)acrylic acid, 0% to 3% by weight of (meth)acrylamide, 0% to 20% by weight of (meth)acrylonitrile, and greater than 0% to less than 50% by weight of a carbohydrate-derived compound having a dextrose equivalent (DE) of about 10 to about 35, based on the total monomer weight;
mixing the aqueous polymer dispersion with a tetrasulfonate-based fluorescent whitening agent to produce a paper coating or binding formulation; and
applying the formulation as a coating to paper.
26. The method according to claim 25, wherein said providing step comprises polymerizing the styrene, butadiene, and itaconic andor (meth)acrylic acid, a and a carbohydrate-derived compound having a dextrose equivalent (DE) of about 10 to about 35, in an aqueous medium to produce the copolymer.
27. The method according to claim 25, wherein the carbohydrate-derived compound is selected from the group consisting of dextrins, maltodextrins, and mixtures thereof.
28. The method according to claim 25, wherein the DE of the carbohydrate-derived compound is from about 12.5 to about 25.
29. The method according to claim 25, wherein the weight average molecular weight of the carbohydrate-derived compound is from about 3000 to about 20,000.
30. The method according to claim 25, wherein the carbohydrate-derived compound is soluble in water at room temperature in an amount of greater than about 40% by weight.
31. The method according to claim 25, wherein the copolymer is derived from about 5 to about 45 percent by weight of the carbohydrate-derived compound based on the total monomer weight.
32. The method according to claim 25, wherein said fluorescent whitening agent is not activated.
33. The method according to claim 25, wherein the formulation is substantially free of polyvinyl alcohol, carboxymethylcellulose, polyvinylpyrrolidone, and water-insoluble starches.
34. Paper comprising a fiber matrix and a binder composition comprising a copolymer derived from 40% to 75% by weight of styrene, 25% to 60% by weight of butadiene, 1% to 10% by weight of itaconic andor (meth)acrylic acid, 0% to 3% by weight of (meth)acrylamide, 0% to 20% by weight of (meth)acrylonitrile, and greater than 0% to less than 50% by weight of a carbohydrate-derived compound having a dextrose equivalent (DE) of about 10 to about 35, based on the total monomer weight, and a tetrasulfonate-based fluorescent whitening agent.
35. Paper according to claim 34, wherein the carbohydrate-derived compound is selected from the group consisting of dextrins, maltodextrins, and mixtures thereof.
36. Paper according to claim 34, wherein the DE of the carbohydrate-derived compound is from about 12.5 to about 25.
37. Paper according to claim 34, wherein the weight average molecular weight of the carbohydrate-derived compound is from about 3,000 to about 20,000.
38. Paper according to claim 34, wherein the carbohydrate-derived compound is soluble in water at room temperature in an amount of greater than about 40% by weight.
39. Paper according to claim 34, wherein the copolymer is derived from about 5 to about 45 percent by weight of the carbohydrate-derived compound based on dry polymer weight.
40. Paper according to claim 34, wherein the fluorescent whitening agent is not activated.
41. Paper according to claim 34, wherein the binder is substantially free of polyvinyl alcohol, carboxymethylcellulose, polyvinylpyrrolidone, and water-insoluble starches.